Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.632 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 152.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 152.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 152.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 165.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 152.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 152.4 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 152.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 152.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 165.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 165.6 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 152.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLaCl5 (mp-772035) | 0.5627 | 0.062 | 3 |
Ba(NaSi2)2 (mp-752573) | 0.4649 | 0.000 | 3 |
BaCaSn3 (mp-583645) | 0.0660 | 0.000 | 3 |
LaSmI4 (mp-570477) | 0.5325 | 0.113 | 3 |
CeNdI4 (mp-570728) | 0.5659 | 0.081 | 3 |
TiTlCuTe3 (mp-9344) | 0.7168 | 0.000 | 4 |
RbHfAgTe3 (mp-9780) | 0.7412 | 0.000 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.7296 | 0.000 | 4 |
MgSi (mp-1073864) | 0.4155 | 0.161 | 2 |
Mg4Si3 (mp-1074349) | 0.4941 | 0.204 | 2 |
Mg4Si3 (mp-1074573) | 0.4330 | 0.202 | 2 |
Mg2Si (mp-1074759) | 0.5026 | 0.174 | 2 |
Mg5Si6 (mp-1075464) | 0.4793 | 0.236 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Yb_2 Sn_d |
Final Energy/Atom-3.7191 eV |
Corrected Energy-148.7642 eV
Uncorrected energy = -148.7642 eV
Corrected energy = -148.7642 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)