Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.605 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 307.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 307.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 247.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 225.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 247.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 123.1 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 246.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 292.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 247.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 157.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 45.0 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 278.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 112.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 90.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 61.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 171.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 202.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 157.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 61.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 270.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 185.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 157.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 45.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 278.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 57.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 283.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 184.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 202.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 180.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 270.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 202.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 22.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 45.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 22.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 57.3 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 221.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 210.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 202.6 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 247.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 180.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 283.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 202.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 157.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 81.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 57.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 294.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 324.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 294.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 231.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K5Hg7 (mp-30718) | 0.6851 | 0.000 | 2 |
UPt2 (mp-30854) | 0.5414 | 0.000 | 2 |
Nb3Ga2 (mp-11393) | 0.6563 | 0.000 | 2 |
Zr3Ga2 (mp-30684) | 0.6581 | 0.000 | 2 |
Ta3Ga2 (mp-16756) | 0.6596 | 0.000 | 2 |
YAlSi (mp-31080) | 0.0888 | 0.000 | 3 |
LuAlSi (mp-567229) | 0.0390 | 0.000 | 3 |
LuAlGe (mp-1025105) | 0.1773 | 0.000 | 3 |
ErAlGe (mp-1024985) | 0.1603 | 0.000 | 3 |
YAlGe (mp-29736) | 0.1476 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points72 |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Al Si |
Final Energy/Atom-5.1565 eV |
Corrected Energy-30.9389 eV
-30.9389 eV = -30.9389 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)