material

Si

ID:

mp-571520

DOI:

10.17188/1276302


Tags: Silicon - XII, HP High pressure experimental phase

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.161 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.161 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.55 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Si
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.002 160.4
SiC (mp-11714) <0 0 1> <0 0 1> 0.002 231.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.004 231.7
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.005 320.8
C (mp-48) <0 0 1> <1 1 0> 0.008 185.2
SiC (mp-8062) <1 1 1> <0 0 1> 0.008 231.7
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.019 213.9
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.021 308.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.021 77.2
Ge (mp-32) <1 1 1> <0 0 1> 0.029 231.7
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.050 92.6
NaCl (mp-22862) <1 0 0> <1 0 0> 0.053 160.4
ZrO2 (mp-2858) <1 1 0> <1 1 0> 0.057 277.8
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.064 320.8
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.068 267.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.073 231.7
GaAs (mp-2534) <1 1 1> <0 0 1> 0.078 231.7
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.080 308.9
BN (mp-984) <0 0 1> <1 0 0> 0.086 267.3
InSb (mp-20012) <1 0 0> <1 0 0> 0.088 267.3
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.090 53.5
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.092 160.4
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.092 231.7
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.093 277.8
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.100 53.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.106 267.3
InSb (mp-20012) <1 1 1> <0 0 1> 0.107 77.2
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.119 231.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.128 77.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.131 320.8
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.134 185.2
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.135 77.2
TiO2 (mp-390) <0 0 1> <1 0 0> 0.142 213.9
Ni (mp-23) <1 1 0> <1 1 0> 0.147 277.8
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.155 267.3
Al (mp-134) <1 0 0> <1 0 0> 0.160 160.4
Al (mp-134) <1 1 1> <1 1 0> 0.160 277.8
CdTe (mp-406) <1 1 0> <1 1 0> 0.160 185.2
Al (mp-134) <1 1 0> <1 1 0> 0.161 92.6
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.163 92.6
InSb (mp-20012) <1 1 0> <1 1 0> 0.168 185.2
GaAs (mp-2534) <1 1 0> <1 1 0> 0.184 92.6
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.184 92.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.193 92.6
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.198 267.3
Cu (mp-30) <1 0 0> <1 0 0> 0.203 320.8
WS2 (mp-224) <1 0 0> <1 0 0> 0.217 267.3
Cu (mp-30) <1 1 0> <1 1 1> 0.227 241.2
NaCl (mp-22862) <1 1 0> <1 1 0> 0.229 92.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.231 160.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
175 39 40 8 10 0
39 175 40 -8 -10 0
40 40 137 0 0 0
8 -8 0 61 0 -10
10 -10 0 0 61 8
0 0 0 -10 8 68
Compliance Tensor Sij (10-12Pa-1)
6.4 -1.2 -1.5 -1 -1.3 0
-1.2 6.4 -1.5 1 1.3 0
-1.5 -1.5 8.2 0 0 0
-1 1 0 17.1 0 2.6
-1.3 1.3 0 0 17.1 -2
0 0 0 2.6 -2 15.3
Shear Modulus GV
63 GPa
Bulk Modulus KV
80 GPa
Shear Modulus GR
60 GPa
Bulk Modulus KR
80 GPa
Shear Modulus GVRH
61 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
0.23
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GaP (mp-971632) 0.4695 0.170 2
AlAs (mp-988945) 0.4671 0.150 2
InAs (mp-20412) 0.4387 0.113 2
GaAs (mp-15619) 0.4629 0.144 2
AlSb (mp-15621) 0.4420 0.117 2
Ge (mp-128) 0.1589 0.148 1
Si (mp-168) 0.5280 0.160 1
Ge (mp-1080106) 0.5404 0.146 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si
Final Energy/Atom
-5.2646 eV
Corrected Energy
-42.1170 eV
Uncorrected energy = -42.1170 eV Corrected energy = -42.1170 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 109036
Submitted by
User remarks:
  • Silicon - XII, HP
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)