Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.541 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnCl2 |
Band Gap4.018 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.0 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 171.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 240.0 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 148.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 240.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 240.0 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 240.0 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 240.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 256.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 256.0 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 256.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 240.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 165.6 |
C (mp-66) | <1 0 0> | <0 1 0> | 256.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 160.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 256.0 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 256.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 234.0 |
Si (mp-149) | <1 1 1> | <0 0 1> | 160.0 |
Au (mp-81) | <1 1 0> | <1 0 -1> | 148.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 240.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 160.0 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 1> | 234.0 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 0> | 256.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 240.0 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 240.0 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 240.0 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 160.0 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 160.0 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 160.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuPO4 (mp-673017) | 0.5798 | 0.129 | 3 |
GaGeS4 (mp-675437) | 0.6160 | 0.167 | 3 |
GaCuI4 (mp-29403) | 0.3365 | 0.000 | 3 |
AlCuCl4 (mp-28020) | 0.3310 | 0.000 | 3 |
GaCuCl4 (mp-29362) | 0.3122 | 0.000 | 3 |
K2Zn(GeO3)2 (mp-560398) | 0.6883 | 0.000 | 4 |
ZnBr2 (mp-647579) | 0.3139 | 0.000 | 2 |
BeCl2 (mp-569030) | 0.3333 | 0.019 | 2 |
BeCl2 (mp-570974) | 0.3276 | 0.009 | 2 |
CeSe2 (mp-1080859) | 0.2840 | 0.505 | 2 |
ZnCl2 (mp-22889) | 0.2366 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Cl |
Final Energy/Atom-2.7971 eV |
Corrected Energy-100.6943 eV
-100.6943 eV = -100.6943 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)