Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.761 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.921 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 206.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 310.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 310.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 310.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 103.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 157.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 310.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 206.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 155.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 206.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 51.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 310.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 206.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 258.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 258.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 206.9 |
BN (mp-984) | <1 1 0> | <1 0 0> | 258.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 310.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 310.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 206.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 142.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 256.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 206.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 310.3 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 310.3 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 0> | 103.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 256.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 310.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 310.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 -1> | 191.5 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 256.6 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 310.3 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 310.3 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 138.3 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 258.6 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 138.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 155.2 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 1> | 157.2 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 310.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 310.3 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 258.6 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 155.2 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 258.6 |
ZnO (mp-2133) | <1 1 1> | <0 1 1> | 190.4 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 310.3 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 140.7 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 206.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.15 | -0.00 | 0.39 |
-0.00 | 9.16 | -0.00 |
0.39 | -0.00 | 4.59 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.09 | -0.00 | 1.52 |
-0.00 | 23.17 | -0.00 |
1.52 | -0.00 | 6.69 |
Polycrystalline dielectric constant
εpoly∞
6.63
|
Polycrystalline dielectric constant
εpoly
13.32
|
Refractive Index n2.58 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaGaBr4 (mp-28679) | 0.7302 | 0.000 | 3 |
NaAlI4 (mp-29395) | 0.7416 | 0.000 | 3 |
Ti4P8S29 (mp-685300) | 0.7129 | 0.001 | 3 |
K2InP2S7 (mp-862780) | 0.4868 | 0.000 | 4 |
TiTlPS5 (mp-558747) | 0.3219 | 0.003 | 4 |
RbTiPS5 (mp-758985) | 0.6442 | 0.000 | 4 |
K4Mn(AsS4)2 (mp-560965) | 0.6774 | 0.035 | 4 |
KTiPS5 (mp-560977) | 0.2158 | 0.000 | 4 |
Sr2ZnNi2(PO4)4 (mvc-15106) | 0.7058 | 0.119 | 5 |
Sr6Li2Cr2N8O (mp-565485) | 0.7266 | 0.246 | 5 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ti_pv P Se |
Final Energy/Atom-4.7480 eV |
Corrected Energy-80.6876 eV
Uncorrected energy = -75.9676 eV
Composition-based energy adjustment (-0.472 eV/atom x 10.0 atoms) = -4.7200 eV
Corrected energy = -80.6876 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)