material

Ba(BiPd)2

ID:

mp-571599

DOI:

10.17188/1272939


Tags: Barium palladium bismuth (1/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.642 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.34 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/m [11]
Hall
-P 2yb
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 416299 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 1 1> <0 0 1> 0.007 197.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.009 197.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.013 197.5
CdWO4 (mp-19387) <1 1 1> <1 1 0> 0.020 155.6
Ni (mp-23) <1 1 0> <1 0 1> 0.035 121.0
MgF2 (mp-1249) <1 0 0> <0 1 1> 0.040 303.3
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.044 222.2
Ga2O3 (mp-886) <1 0 0> <0 1 1> 0.046 182.0
C (mp-48) <1 0 0> <0 0 1> 0.046 271.5
C (mp-48) <1 1 1> <1 0 1> 0.047 302.4
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.049 197.5
CsI (mp-614603) <1 0 0> <0 0 1> 0.049 123.4
Ni (mp-23) <1 0 0> <0 0 1> 0.052 24.7
Te2W (mp-22693) <0 0 1> <0 0 1> 0.057 222.2
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.060 197.5
InP (mp-20351) <1 0 0> <0 0 1> 0.060 320.9
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.062 123.4
C (mp-48) <0 0 1> <0 0 1> 0.063 271.5
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.069 123.4
TeO2 (mp-2125) <0 1 0> <1 0 0> 0.072 272.9
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.076 123.4
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.078 123.4
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.078 222.2
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.081 222.2
Al (mp-134) <1 1 0> <0 0 1> 0.083 320.9
GaN (mp-804) <1 1 1> <0 0 1> 0.092 123.4
GaN (mp-804) <1 0 0> <0 1 0> 0.092 221.6
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.097 272.9
InSb (mp-20012) <1 0 0> <0 0 1> 0.098 222.2
TiO2 (mp-2657) <1 0 1> <0 1 1> 0.105 182.0
CdTe (mp-406) <1 0 0> <0 0 1> 0.112 222.2
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.122 345.6
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.125 271.5
GaSe (mp-1943) <1 0 1> <0 1 0> 0.134 277.0
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.139 327.5
Ag (mp-124) <1 0 0> <0 0 1> 0.145 222.2
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.146 302.4
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.150 197.5
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.151 123.4
Te2W (mp-22693) <0 1 0> <0 0 1> 0.153 320.9
ZnO (mp-2133) <1 0 1> <0 0 1> 0.159 320.9
AlN (mp-661) <1 0 0> <1 0 0> 0.168 109.2
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.168 222.2
BN (mp-984) <1 0 1> <0 1 0> 0.177 277.0
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.180 327.5
CdWO4 (mp-19387) <0 1 1> <0 1 1> 0.181 121.3
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.185 302.4
Ga2O3 (mp-886) <1 0 1> <1 0 1> 0.192 181.5
Ag (mp-124) <1 1 1> <0 0 1> 0.195 148.1
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.202 54.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
82 47 51 0 0 0
47 90 41 0 3 0
51 41 88 0 -4 0
0 0 0 19 0 4
0 3 -4 0 22 0
0 0 0 4 0 19
Compliance Tensor Sij (10-12Pa-1)
22.4 -7.4 -9.6 0 -0.9 0
-7.4 16.8 -3.6 0 -2.8 0
-9.6 -3.6 18.8 0 3.8 0
0 0 0 56.3 0 -12.3
-0.9 -2.8 3.8 0 46.2 0
0 0 0 -12.3 0 54.6
Shear Modulus GV
20 GPa
Bulk Modulus KV
60 GPa
Shear Modulus GR
19 GPa
Bulk Modulus KR
60 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
60 GPa
Elastic Anisotropy
0.25
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sm(NiBi)2 (mp-978997) 0.5005 0.110 3
Nd(NiBi)2 (mp-976277) 0.5020 0.074 3
Sr(BiPd)2 (mp-567114) 0.1697 0.000 3
Ba(SbAu)2 (mp-570298) 0.3552 0.000 3
BaSn3Au (mp-1068048) 0.5016 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Bi Pd
Final Energy/Atom
-4.6542 eV
Corrected Energy
-46.5423 eV
-46.5423 eV = -46.5423 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 416299
Submitted by
User remarks:
  • Barium palladium bismuth (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)