Final Magnetic Moment0.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.133 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaTb2O4 + BaO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 67.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 314.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 167.9 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 135.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 331.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 196.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 335.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 263.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 55.3 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 276.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 331.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 314.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 55.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 196.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 157.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.7 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 135.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 314.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 165.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 110.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 196.6 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 196.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 135.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 196.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 353.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 196.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 196.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 196.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 221.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 203.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 275.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 279.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 165.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 275.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 314.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 55.3 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 276.6 |
BN (mp-984) | <0 0 1> | <0 1 1> | 135.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 314.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 196.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 275.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 236.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 223.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 135.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 279.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrSnO3 (mp-12866) | 0.0817 | 0.006 | 3 |
LaGaO3 (mp-556983) | 0.0744 | 0.038 | 3 |
CaTiO3 (mp-556003) | 0.0930 | 0.011 | 3 |
BaCeO3 (mp-3316) | 0.0561 | 0.001 | 3 |
SrZrO3 (mp-1080575) | 0.0868 | 0.006 | 3 |
CaLaMn2O6 (mp-25765) | 0.2807 | 0.109 | 4 |
YSb(PbO3)2 (mp-1078392) | 0.2956 | 0.022 | 4 |
Sr2TaInO6 (mp-1078748) | 0.1862 | 0.000 | 4 |
Ba2NdBiO6 (mp-546321) | 0.2896 | 0.000 | 4 |
Ba2LaBiO6 (mp-1078409) | 0.2885 | 0.000 | 4 |
Pb3O4 (mp-636813) | 0.7397 | 0.038 | 2 |
NaLa2Ti2MnO9 (mp-694960) | 0.3205 | 0.228 | 5 |
NaNd3Ti3MnO12 (mp-694881) | 0.3205 | 0.216 | 5 |
Na5Ce3Ti6Nb2O24 (mp-691045) | 0.2840 | 0.000 | 5 |
SrLiPrTeO6 (mp-39144) | 0.2984 | 0.023 | 5 |
CaLaMnFeO6 (mp-41963) | 0.3422 | 0.065 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Tb_3 O |
Final Energy/Atom-6.9913 eV |
Corrected Energy-74.0350 eV
Uncorrected energy = -69.9130 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -74.0350 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)