Final Magnetic Moment1.377 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.989 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 52.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 218.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 75.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 260.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 260.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 186.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 260.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 210.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 160.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.2 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 210.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 240.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 240.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 195.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 223.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 60.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 135.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 135.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 255.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 111.6 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 105.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 186.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 160.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 260.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 240.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 186.0 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 120.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 75.2 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 135.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 240.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 270.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 45.1 |
MoS2 (mp-1434) | <1 0 1> | <1 1 1> | 273.6 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 120.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 135.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 255.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 195.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 225.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 135.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 280.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 200.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 1> | 164.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 45.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 148.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 297.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 263.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 195.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
256 | 41 | 64 | 0 | 0 | 0 |
41 | 256 | 64 | 0 | 0 | 0 |
64 | 64 | 156 | 0 | 0 | 0 |
0 | 0 | 0 | 111 | 0 | 0 |
0 | 0 | 0 | 0 | 111 | 0 |
0 | 0 | 0 | 0 | 0 | 101 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.4 | -0.3 | -1.7 | 0 | 0 | 0 |
-0.3 | 4.4 | -1.7 | 0 | 0 | 0 |
-1.7 | -1.7 | 7.8 | 0 | 0 | 0 |
0 | 0 | 0 | 9 | 0 | 0 |
0 | 0 | 0 | 0 | 9 | 0 |
0 | 0 | 0 | 0 | 0 | 9.9 |
Shear Modulus GV98 GPa |
Bulk Modulus KV112 GPa |
Shear Modulus GR91 GPa |
Bulk Modulus KR108 GPa |
Shear Modulus GVRH94 GPa |
Bulk Modulus KVRH110 GPa |
Elastic Anisotropy0.39 |
Poisson's Ratio0.17 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(CoP)2 (mp-3210) | 0.0433 | 0.000 | 3 |
Ce(CoSi)2 (mp-3437) | 0.0598 | 0.000 | 3 |
Nd(NiAs)2 (mp-567723) | 0.0602 | 0.028 | 3 |
Sm(NiAs)2 (mp-567818) | 0.0367 | 0.028 | 3 |
Gd(NiAs)2 (mp-582433) | 0.0456 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.5375 | 0.000 | 4 |
ThZn4 (mp-536) | 0.2328 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.2301 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.2121 | 0.000 | 2 |
BaIn4 (mp-22687) | 0.2407 | 0.000 | 2 |
BaGa4 (mp-335) | 0.2409 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Co P |
Final Energy/Atom-6.9416 eV |
Corrected Energy-34.7080 eV
Uncorrected energy = -34.7080 eV
Corrected energy = -34.7080 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)