material

HfAlNi2

ID:

mp-5748

DOI:

10.17188/1276596


Tags: Aluminium hafnium nickel (1/1/2)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.637 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 57901 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 0 0> <1 0 0> 0.000 296.0
Ni (mp-23) <1 1 0> <1 1 0> 0.003 52.3
Ni (mp-23) <1 1 1> <1 1 1> 0.003 64.1
C (mp-66) <1 0 0> <1 0 0> 0.004 332.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.006 296.0
SiC (mp-11714) <0 0 1> <1 1 1> 0.006 256.3
SiC (mp-7631) <0 0 1> <1 1 1> 0.009 256.3
LiGaO2 (mp-5854) <1 1 0> <1 1 1> 0.014 192.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.024 296.0
Ag (mp-124) <1 0 0> <1 0 0> 0.025 296.0
AlN (mp-661) <0 0 1> <1 0 0> 0.029 296.0
Al (mp-134) <1 0 0> <1 0 0> 0.048 148.0
Al (mp-134) <1 1 0> <1 1 0> 0.049 209.3
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.058 157.0
GaN (mp-804) <1 0 0> <1 0 0> 0.073 185.0
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.075 296.0
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.077 256.3
Ge (mp-32) <1 0 0> <1 0 0> 0.077 296.0
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.078 256.3
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.079 148.0
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.084 157.0
LaF3 (mp-905) <1 0 0> <1 1 1> 0.087 320.4
Si (mp-149) <1 0 0> <1 0 0> 0.087 148.0
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.109 148.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.111 209.3
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.128 209.3
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.129 222.0
ZnO (mp-2133) <0 0 1> <1 1 1> 0.137 256.3
Ni (mp-23) <1 0 0> <1 1 0> 0.137 261.6
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.139 209.3
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.151 185.0
Mg (mp-153) <1 0 0> <1 0 0> 0.152 185.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.156 148.0
LiF (mp-1138) <1 1 0> <1 1 0> 0.160 209.3
LiF (mp-1138) <1 1 1> <1 1 1> 0.161 256.3
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.161 256.3
BN (mp-984) <0 0 1> <1 0 0> 0.166 259.0
NaCl (mp-22862) <1 0 0> <1 0 0> 0.172 296.0
Mg (mp-153) <1 1 0> <1 1 0> 0.191 313.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.195 259.0
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.195 74.0
SiC (mp-11714) <1 0 1> <1 0 0> 0.199 259.0
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.200 104.6
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.214 259.0
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.227 256.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.233 332.9
Cu (mp-30) <1 0 0> <1 0 0> 0.253 332.9
ZnO (mp-2133) <1 0 1> <1 0 0> 0.261 222.0
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.272 192.2
SiC (mp-11714) <1 0 0> <1 0 0> 0.277 185.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
218 138 138 0 0 0
138 218 138 0 0 0
138 138 218 0 0 0
0 0 0 56 0 0
0 0 0 0 56 0
0 0 0 0 0 56
Compliance Tensor Sij (10-12Pa-1)
8.9 -3.5 -3.5 0 0 0
-3.5 8.9 -3.5 0 0 0
-3.5 -3.5 8.9 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 18
Shear Modulus GV
49 GPa
Bulk Modulus KV
164 GPa
Shear Modulus GR
48 GPa
Bulk Modulus KR
164 GPa
Shear Modulus GVRH
49 GPa
Bulk Modulus KVRH
164 GPa
Elastic Anisotropy
0.12
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
VGaFe2 (mp-21883) 0.0000 0.000 3
MnInPd2 (mp-31328) 0.0000 0.000 3
Li2SbAu (mp-30404) 0.0000 0.000 3
NbAlCo2 (mp-5149) 0.0000 0.009 3
SmMg2Ag (mp-11235) 0.0000 0.168 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Rb3Bi (mp-23304) 0.0000 0.028 2
Sr3In (mp-31349) 0.0000 0.131 2
Fe3Ge (mp-20711) 0.0000 0.000 2
LiGa (mp-1307) 0.0000 0.000 2
NaTl (mp-1564) 0.0000 0.000 2
Eu (mp-20071) 0.0000 0.085 1
Ba (mp-122) 0.0000 0.000 1
Ce (mp-10024) 0.0000 0.228 1
Np (mp-10207) 0.0000 0.447 1
Gd (mp-11421) 0.0000 0.088 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Al Ni_pv
Final Energy/Atom
-6.9522 eV
Corrected Energy
-27.8089 eV
-27.8089 eV = -27.8089 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 608123
  • 57901
Submitted by
User remarks:
  • Aluminium hafnium nickel (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)