material

Cu3PSe4

ID:

mp-5756

DOI:

10.17188/1276599


Tags: Tricopper(I) tetraselenophosphate(V) Tricopper(I) tetraselenophosphate

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.376 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.32 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.048 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmn21 [31]
Hall
P 2ac 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 2856 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 1 1> <1 0 1> 0.002 271.1
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.002 208.7
Si (mp-149) <1 1 1> <0 0 1> 0.014 259.6
C (mp-66) <1 0 0> <1 0 1> 0.014 203.4
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.015 259.6
Ag (mp-124) <1 1 1> <1 0 0> 0.016 208.7
SiC (mp-11714) <1 1 0> <1 0 1> 0.018 271.1
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.020 346.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.021 208.7
SiC (mp-11714) <0 0 1> <1 0 0> 0.024 208.7
C (mp-48) <1 1 0> <0 1 0> 0.026 99.7
GaN (mp-804) <0 0 1> <0 0 1> 0.028 216.4
Ga2O3 (mp-886) <1 0 0> <0 1 1> 0.032 198.1
LiGaO2 (mp-5854) <0 1 0> <0 1 1> 0.037 66.0
C (mp-48) <0 0 1> <0 0 1> 0.042 173.1
KCl (mp-23193) <1 1 0> <0 0 1> 0.047 173.1
LiF (mp-1138) <1 1 0> <0 0 1> 0.048 259.6
GaN (mp-804) <1 1 0> <0 1 0> 0.051 349.0
Te2Mo (mp-602) <1 1 1> <1 1 0> 0.051 288.7
Au (mp-81) <1 1 1> <1 0 0> 0.058 208.7
WS2 (mp-224) <0 0 1> <0 1 0> 0.059 249.3
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.060 249.3
ZnO (mp-2133) <1 0 1> <1 1 0> 0.060 216.5
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.065 216.5
LaF3 (mp-905) <1 0 1> <1 0 0> 0.070 208.7
YAlO3 (mp-3792) <0 0 1> <0 1 1> 0.073 198.1
SiC (mp-11714) <1 0 0> <0 1 0> 0.075 249.3
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.083 259.6
GaP (mp-2490) <1 1 1> <0 0 1> 0.083 259.6
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.085 208.7
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.088 346.2
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.094 346.2
CsI (mp-614603) <1 1 0> <1 0 0> 0.096 260.9
YAlO3 (mp-3792) <0 1 1> <1 1 0> 0.099 144.3
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.101 208.7
BaTiO3 (mp-5986) <1 1 1> <0 1 0> 0.102 199.4
Si (mp-149) <1 0 0> <0 1 1> 0.105 330.1
WSe2 (mp-1821) <1 0 0> <1 0 1> 0.105 203.4
CeO2 (mp-20194) <1 0 0> <0 1 1> 0.107 330.1
AlN (mp-661) <1 0 0> <0 1 0> 0.107 249.3
ZnO (mp-2133) <1 1 1> <1 1 1> 0.107 252.4
LiTaO3 (mp-3666) <1 1 0> <1 1 1> 0.107 252.4
Mg (mp-153) <0 0 1> <0 1 0> 0.112 249.3
YVO4 (mp-19133) <1 1 0> <0 1 1> 0.113 66.0
Al (mp-134) <1 0 0> <1 0 0> 0.115 313.0
KCl (mp-23193) <1 0 0> <0 1 0> 0.118 249.3
ZrO2 (mp-2858) <1 0 0> <0 1 1> 0.119 198.1
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.122 302.9
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.124 313.0
Cu (mp-30) <1 0 0> <0 1 0> 0.129 199.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
102 50 38 0 0 0
50 99 36 0 0 0
38 36 129 0 0 0
0 0 0 24 0 0
0 0 0 0 24 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
13.5 -5.9 -2.3 0 0 0
-5.9 13.8 -2.1 0 0 0
-2.3 -2.1 9 0 0 0
0 0 0 42.4 0 0
0 0 0 0 42.5 0
0 0 0 0 0 38.2
Shear Modulus GV
28 GPa
Bulk Modulus KV
64 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
64 GPa
Shear Modulus GVRH
28 GPa
Bulk Modulus KVRH
64 GPa
Elastic Anisotropy
0.28
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cu3PS4 (mp-3934) 0.1701 0.000 3
Cu2SnS3 (mp-10519) 0.1619 0.000 3
Cu2SiS3 (mp-15895) 0.1495 0.009 3
Cu3SbS4 (mp-5702) 0.1728 0.000 3
Cu2SiS3 (mp-561468) 0.1419 0.135 3
ZnCu2SiS4 (mp-977414) 0.1126 0.002 4
Cu4Si2NiS7 (mp-557274) 0.1442 0.024 4
FeCu2SnS4 (mp-628568) 0.1665 0.043 4
Ag2SnHgSe4 (mp-10963) 0.0688 0.000 4
MnCu2GeS4 (mp-20474) 0.0988 0.000 4
CuI (mp-673245) 0.1908 0.008 2
BC7 (mp-1080030) 0.2199 0.249 2
BC5 (mp-1018649) 0.2052 0.278 2
BC7 (mp-1079661) 0.2307 0.244 2
BC5 (mp-1095514) 0.1622 0.302 2
Sn (mp-949028) 0.1767 0.030 1
Si (mp-971662) 0.1757 0.064 1
C (mp-569517) 0.3104 0.145 1
C (mp-611426) 0.3076 0.146 1
Ge (mp-1091415) 0.3042 0.014 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv P Se
Final Energy/Atom
-4.1016 eV
Corrected Energy
-69.4014 eV
Uncorrected energy = -65.6254 eV Composition-based energy adjustment (-0.472 eV/atom x 8.0 atoms) = -3.7760 eV Corrected energy = -69.4014 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 2856
  • 41906
  • 95412
Submitted by
User remarks:
  • Tricopper(I) tetraselenophosphate(V)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)