Final Magnetic Moment6.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.123 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 253.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 284.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 253.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 253.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 284.2 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 284.2 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 253.9 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 284.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 221.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 253.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 284.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 169.3 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 253.9 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 253.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 253.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 253.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 253.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 253.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 284.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 284.2 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 284.2 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 253.9 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 169.3 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 1> | 221.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 253.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 284.2 |
TiO2 (mp-390) | <1 0 0> | <0 1 1> | 110.5 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 284.2 |
C (mp-48) | <1 1 0> | <0 1 0> | 169.3 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 213.2 |
ZnO (mp-2133) | <1 0 1> | <0 1 1> | 221.0 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 253.9 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 284.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 284.2 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 1> | 221.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3(W3O8)4 (mp-780475) | 0.5877 | 0.031 | 3 |
BaTa6O16 (mp-769349) | 0.5621 | 0.000 | 3 |
Nb5O12F (mp-759636) | 0.6546 | 0.043 | 3 |
Ta2WO8 (mp-773933) | 0.3486 | 0.003 | 3 |
Nb6CdO16 (mp-773090) | 0.5847 | 0.049 | 3 |
U2O5 (mp-647814) | 0.4650 | 0.017 | 2 |
U13O34 (mp-642328) | 0.6529 | 0.017 | 2 |
W18O49 (mp-19529) | 0.2262 | 0.000 | 2 |
W18O49 (mp-567091) | 0.2272 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: W_pv O |
Final Energy/Atom-7.5716 eV |
Corrected Energy-1076.5338 eV
-1076.5338 eV = -878.3095 eV (uncorrected energy) - 139.2320 eV (MP Advanced Correction) - 58.9924 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)