Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.151 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.040 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2CuP2O7 + CuO |
Band Gap0.004 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 238.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 215.8 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 178.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 215.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 177.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 297.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 190.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 190.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 333.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 283.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 238.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 86.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 215.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 212.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 354.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 215.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 172.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 240.6 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 190.8 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 258.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 212.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 333.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 190.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 297.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 212.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 283.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 287.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 215.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 248.1 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 106.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 319.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 106.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 70.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 177.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 319.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 141.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 212.7 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 297.1 |
GaSe (mp-1943) | <1 0 0> | <1 1 1> | 279.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 354.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 333.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 177.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 215.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 238.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 238.5 |
BN (mp-984) | <1 1 0> | <0 1 1> | 297.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 237.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 212.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 354.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 141.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.02561 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.04822 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.19529 |
Piezoelectric Modulus ‖eij‖max0.19529 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.60 | 0.00 | 0.00 |
0.00 | 4.51 | 0.00 |
0.00 | 0.00 | 4.27 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.51 | 0.00 | 0.00 |
0.00 | 9.18 | 0.00 |
0.00 | 0.00 | 9.92 |
Polycrystalline dielectric constant
εpoly∞
4.13
|
Polycrystalline dielectric constant
εpoly
8.87
|
Refractive Index n2.03 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs3HoO3 (mp-768211) | 0.7292 | 0.000 | 3 |
AlBiO3 (mvc-3494) | 0.7146 | 0.518 | 3 |
Rb3TmO3 (mp-752406) | 0.7277 | 0.002 | 3 |
Rb3ErO3 (mp-756812) | 0.7322 | 0.005 | 3 |
Sr2VO4 (mp-554926) | 0.6930 | 0.043 | 3 |
LiFePO4 (mp-766762) | 0.5925 | 0.544 | 4 |
LiSiBiO4 (mp-766176) | 0.5927 | 0.028 | 4 |
LiCoPO4 (mp-765449) | 0.5491 | 0.082 | 4 |
LiMnPO4 (mp-31994) | 0.4307 | 0.038 | 4 |
LiFePO4 (mp-761476) | 0.5497 | 0.063 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Cu_pv P O |
Final Energy/Atom-6.1231 eV |
Corrected Energy-182.4388 eV
Uncorrected energy = -171.4468 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Corrected energy = -182.4388 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)