Final Magnetic Moment0.229 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.684 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/m [176] |
Hall-P 6c |
Point Group6/m |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 254.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 254.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 84.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 169.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 84.7 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 169.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 84.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 254.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 84.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 254.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 254.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 169.3 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 84.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 254.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 254.0 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 254.0 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 169.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 254.0 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 254.0 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 254.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsMo6Se7 (mp-5883) | 0.3510 | 0.012 | 3 |
CsTe7Mo6 (mp-18193) | 0.3555 | 0.000 | 3 |
Rb2Mo9Se10 (mp-542629) | 0.1754 | 0.004 | 3 |
Cs2Te10Mo9 (mp-581150) | 0.2921 | 0.000 | 3 |
Rb5Mo18S19 (mp-669350) | 0.3496 | 0.004 | 3 |
Mo9Se11 (mp-638048) | 0.5708 | 0.065 | 2 |
Mo9Se11 (mp-299) | 0.6121 | 0.081 | 2 |
Mo15Se19 (mp-568488) | 0.6689 | 0.065 | 2 |
Mo15Se19 (mp-570170) | 0.6106 | 0.064 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Mo_pv Se |
Final Energy/Atom-7.0647 eV |
Corrected Energy-692.3430 eV
-692.3430 eV = -692.3430 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)