Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.798 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.774 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 312.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 234.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 312.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 234.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 312.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 234.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 234.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 312.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 312.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 78.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 234.4 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 312.5 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 234.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 312.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 312.5 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 312.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 312.5 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 234.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 234.4 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 312.5 |
C (mp-48) | <1 0 0> | <0 0 1> | 78.1 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 312.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 312.5 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 234.4 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 312.5 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 197.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 234.4 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 312.5 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 156.3 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 156.3 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 156.3 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 312.5 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 156.3 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 156.3 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 312.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 234.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 312.5 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 234.4 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 312.5 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 312.5 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 156.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 312.5 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 312.5 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 312.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlGeS2 (mp-3075) | 0.6283 | 0.000 | 3 |
KPSe3 (mp-571452) | 0.6660 | 0.002 | 3 |
Bi2(PSe3)3 (mp-569308) | 0.6405 | 0.004 | 3 |
KPSe3 (mp-569702) | 0.6497 | 0.000 | 3 |
Sb2(PSe3)3 (mp-15046) | 0.6839 | 0.000 | 3 |
NaSb(PS3)2 (mp-561303) | 0.6530 | 0.007 | 4 |
Rb2HgPSe5 (mp-569349) | 0.5897 | 0.000 | 4 |
Cs2AgAsS4 (mp-561622) | 0.6146 | 0.000 | 4 |
Cs2AgSbS4 (mp-510710) | 0.5865 | 0.000 | 4 |
AgBi(PS3)2 (mp-556434) | 0.5607 | 0.000 | 4 |
Tl4Hg3Sb2(As2S5)4 (mp-553948) | 0.7382 | 0.011 | 5 |
K4GeH4N2O3 (mp-720197) | 0.7240 | 0.000 | 5 |
K3GeH2NO3 (mp-697540) | 0.5736 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Ge_d As Se |
Final Energy/Atom-3.7394 eV |
Corrected Energy-149.5771 eV
-149.5771 eV = -149.5771 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)