LiSi2N3

ID:

mp-5853

DOI:

10.17188/1277112


Tags: Lithium disilicon nitride Lithium trinitridodisilicatee

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.337 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
5.018 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmc21 [36]
Hall
C 2c 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 34118 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.009 346.2
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.011 98.9
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.013 247.3
TePb (mp-19717) <1 0 0> <0 0 1> 0.019 346.2
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.022 268.0
C (mp-66) <1 0 0> <1 0 1> 0.022 333.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.028 49.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.032 49.5
TePb (mp-19717) <1 1 1> <0 0 1> 0.035 148.4
MoS2 (mp-1434) <1 0 0> <0 1 0> 0.040 205.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.043 98.9
Al2O3 (mp-1143) <0 0 1> <0 1 0> 0.049 282.3
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.074 312.6
LaF3 (mp-905) <1 0 0> <1 0 1> 0.081 266.5
MoS2 (mp-1434) <1 0 1> <0 1 0> 0.083 205.3
Cu (mp-30) <1 1 0> <1 0 1> 0.086 333.2
ZnO (mp-2133) <0 0 1> <1 1 1> 0.094 214.2
YAlO3 (mp-3792) <0 0 1> <0 1 1> 0.107 55.7
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.116 256.7
CdTe (mp-406) <1 1 0> <0 0 1> 0.118 247.3
InSb (mp-20012) <1 1 0> <0 0 1> 0.129 247.3
SiC (mp-7631) <1 0 0> <0 1 0> 0.130 282.3
AlN (mp-661) <1 0 0> <1 0 0> 0.141 268.0
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.142 134.0
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.148 197.8
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.160 154.5
Ni (mp-23) <1 0 0> <0 1 1> 0.161 111.4
LaAlO3 (mp-2920) <1 1 0> <0 0 1> 0.163 247.3
Te2Mo (mp-602) <1 0 0> <1 0 1> 0.173 333.2
SrTiO3 (mp-4651) <1 1 1> <0 1 0> 0.177 205.3
CdS (mp-672) <1 0 0> <1 1 1> 0.183 142.8
CdWO4 (mp-19387) <0 1 1> <0 1 0> 0.205 205.3
LiTaO3 (mp-3666) <0 0 1> <0 1 1> 0.211 278.6
WS2 (mp-224) <0 0 1> <0 1 0> 0.218 282.3
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.218 282.3
CdS (mp-672) <0 0 1> <0 1 0> 0.220 256.7
GaTe (mp-542812) <1 0 0> <0 1 1> 0.221 222.9
Mg (mp-153) <0 0 1> <0 1 0> 0.237 282.3
TiO2 (mp-390) <1 1 0> <0 1 0> 0.240 51.3
KP(HO2)2 (mp-23959) <0 1 0> <1 1 0> 0.243 154.5
Al2O3 (mp-1143) <1 0 0> <0 1 0> 0.248 128.3
SiC (mp-11714) <1 0 1> <0 1 1> 0.258 222.9
GaN (mp-804) <1 0 0> <0 1 0> 0.260 51.3
GaN (mp-804) <1 1 0> <0 0 1> 0.263 148.4
Ni (mp-23) <1 1 0> <0 0 1> 0.263 247.3
Fe2O3 (mp-24972) <0 0 1> <0 1 1> 0.268 278.6
BN (mp-984) <1 1 0> <0 1 1> 0.271 167.1
YVO4 (mp-19133) <1 0 1> <0 1 0> 0.277 205.3
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.283 247.3
KP(HO2)2 (mp-23959) <0 0 1> <1 1 0> 0.295 154.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
304 79 63 0 0 0
79 342 67 0 0 0
63 67 366 0 0 0
0 0 0 104 0 0
0 0 0 0 134 0
0 0 0 0 0 107
Compliance Tensor Sij (10-12Pa-1)
3.6 -0.7 -0.5 0 0 0
-0.7 3.2 -0.5 0 0 0
-0.5 -0.5 2.9 0 0 0
0 0 0 9.6 0 0
0 0 0 0 7.5 0
0 0 0 0 0 9.4
Shear Modulus GV
122 GPa
Bulk Modulus KV
159 GPa
Shear Modulus GR
120 GPa
Bulk Modulus KR
158 GPa
Shear Modulus GVRH
121 GPa
Bulk Modulus KVRH
159 GPa
Elastic Anisotropy
0.09
Poisson's Ratio
0.20

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.08082 0.00000
0.00000 0.00000 0.00000 -0.42772 0.00000 0.00000
-0.16085 -0.44966 0.77927 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.91396 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.36 0.00 0.00
0.00 4.50 0.00
0.00 0.00 4.35
Dielectric Tensor εij (total)
8.75 0.00 0.00
0.00 12.04 0.00
0.00 0.00 9.99
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.41
Polycrystalline dielectric constant εpoly
(total)
10.26
Refractive Index n
2.10
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiAgF2 (mp-752882) 0.4284 0.051 3
NaCo3O4 (mp-763987) 0.3871 0.819 3
NaFeO2 (mp-24939) 0.4439 0.050 3
NaGe2N3 (mp-14433) 0.3796 0.000 3
NaFeO2 (mp-566778) 0.4404 0.050 3
Li2AlFeO4 (mp-770733) 0.3771 0.304 4
Li2AlFeO4 (mp-770704) 0.3745 0.310 4
Li2AlCoO4 (mp-770610) 0.3754 0.308 4
Li2AlNiO4 (mp-770400) 0.3700 0.169 4
Li2AlCoO4 (mp-771906) 0.3794 0.219 4
CdP2 (mp-913) 0.6792 0.000 2
CdP2 (mp-12112) 0.6782 0.000 2
Si (mp-16220) 0.7423 0.338 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Si N
Final Energy/Atom
-7.4392 eV
Corrected Energy
-89.2705 eV
-89.2705 eV = -89.2705 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 34118
  • 89524
Submitted by
User remarks:
  • Lithium disilicon nitride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)