Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.147 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 247.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 272.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 297.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 198.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 321.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 346.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 371.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 198.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 148.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 371.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 247.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 123.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 272.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 173.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 198.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 321.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 272.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 297.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 173.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 123.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 148.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 272.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 272.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 346.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 173.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 222.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 297.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 173.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 123.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 24.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 173.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 198.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 163.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 247.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 321.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 99.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 173.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 123.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 346.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 272.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 297.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 173.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 247.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 272.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 272.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 247.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zr2CoP (mp-29152) | 0.6254 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.6478 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.6780 | 0.000 | 3 |
LaTeAs (mp-10383) | 0.7137 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.5569 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.6357 | 0.106 | 4 |
YCo (mp-8053) | 0.3151 | 0.004 | 2 |
CaCu (mp-30471) | 0.0635 | 0.001 | 2 |
BaAg (mp-11840) | 0.3553 | 0.000 | 2 |
YbNi (mp-1080433) | 0.3263 | 0.023 | 2 |
EuCu (mp-1087547) | 0.3052 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Cu_pv |
Final Energy/Atom-3.1961 eV |
Corrected Energy-127.8432 eV
-127.8432 eV = -127.8432 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)