Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.490 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <1 1 1> | 184.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 106.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 184.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 212.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 212.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 212.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 212.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.3 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 184.1 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 184.1 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 150.3 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 184.1 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 150.3 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 184.1 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 212.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 184.1 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 106.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 150.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ta2Cd2O7 (mp-5548) | 0.0239 | 0.000 | 3 |
Ca2Nb2O7 (mp-4155) | 0.0078 | 0.042 | 3 |
Nb2Cd2O7 (mp-5472) | 0.0095 | 0.010 | 3 |
Ca2Ru2O7 (mp-554638) | 0.0315 | 0.000 | 3 |
Ca2Ta2O7 (mp-14026) | 0.0161 | 0.001 | 3 |
Mn2Hg2SF6 (mp-600275) | 0.2657 | 0.000 | 4 |
Cu2Hg2SF6 (mp-6820) | 0.0265 | 0.000 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.2751 | 0.000 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.1851 | 0.000 | 4 |
Ni2Hg2SF6 (mp-559259) | 0.0556 | 0.000 | 4 |
YbTiCdSbO7 (mp-677151) | 0.3405 | 0.065 | 5 |
NaCaNb2O6F (mp-42255) | 0.2255 | 0.005 | 5 |
LiCaTa2O6F (mp-39511) | 0.1553 | 0.030 | 5 |
Ca2Nd2Nb3FeO14 (mvc-16570) | 0.3079 | 0.027 | 5 |
Ca2Nd2Nb3FeO14 (mp-40206) | 0.2678 | 0.027 | 5 |
NaYbTiNbO6F (mp-684861) | 0.3873 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.4783 | 0.036 | 6 |
NaEuTiNbO6F (mp-43048) | 0.3675 | 0.012 | 6 |
NaCeTiNbO6F (mp-43055) | 0.4639 | 0.033 | 6 |
NaNdTiNbO6F (mp-43134) | 0.4751 | 0.037 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: O Cd Os_pv |
Final Energy/Atom-6.3902 eV |
Corrected Energy-150.4163 eV
-150.4163 eV = -140.5842 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)