material

YBPt2

ID:

mp-5971

DOI:

10.17188/1277208


Tags: Yttrium platinum boride (1/2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.002 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.27 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6222 [180]
Hall
P 62 2c (0 0 1)
Point Group
622
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 156946 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <0 0 1> 0.000 24.9
SiC (mp-7631) <0 0 1> <0 0 1> 0.000 24.9
TePb (mp-19717) <1 1 1> <0 0 1> 0.000 74.6
SiC (mp-8062) <1 1 1> <0 0 1> 0.002 99.5
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.003 128.5
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.003 323.4
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.009 296.8
Fe2O3 (mp-24972) <0 0 1> <1 1 0> 0.009 296.8
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.009 296.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.018 223.9
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.019 128.5
C (mp-48) <0 0 1> <0 0 1> 0.042 99.5
C (mp-66) <1 0 0> <1 0 0> 0.042 128.5
InP (mp-20351) <1 0 0> <1 0 0> 0.046 214.2
TeO2 (mp-2125) <1 1 0> <1 1 0> 0.049 296.8
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.064 174.1
NaCl (mp-22862) <1 0 0> <1 0 0> 0.066 128.5
Cu (mp-30) <1 1 1> <1 1 0> 0.068 296.8
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.075 222.6
Ge (mp-32) <1 1 1> <0 0 1> 0.076 174.1
TiO2 (mp-390) <0 0 1> <1 0 1> 0.081 247.7
PbS (mp-21276) <1 0 0> <1 0 0> 0.085 214.2
TePb (mp-19717) <1 0 0> <1 0 1> 0.087 346.8
SiC (mp-7631) <1 1 1> <1 0 1> 0.094 247.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.103 128.5
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.105 214.2
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.116 323.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.119 128.5
C (mp-48) <1 0 1> <1 0 0> 0.130 257.1
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.135 222.6
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.139 257.1
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.140 323.4
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.149 323.4
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.155 198.2
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.157 198.2
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.165 323.4
GaAs (mp-2534) <1 1 1> <0 0 1> 0.168 174.1
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.176 174.1
TiO2 (mp-390) <1 1 1> <1 0 0> 0.182 214.2
SiC (mp-11714) <1 1 0> <1 0 0> 0.202 214.2
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.206 124.4
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.207 128.5
C (mp-48) <1 1 1> <1 0 0> 0.214 171.4
Al (mp-134) <1 0 0> <1 0 0> 0.215 128.5
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.215 74.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.226 223.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.227 223.9
AlN (mp-661) <1 1 0> <1 0 0> 0.231 214.2
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.241 257.1
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.242 174.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
241 124 123 0 0 0
124 241 123 0 0 0
123 123 213 0 0 0
0 0 0 46 0 0
0 0 0 0 46 0
0 0 0 0 0 58
Compliance Tensor Sij (10-12Pa-1)
6.5 -2 -2.6 0 0 0
-2 6.5 -2.6 0 0 0
-2.6 -2.6 7.7 0 0 0
0 0 0 21.8 0 0
0 0 0 0 21.8 0
0 0 0 0 0 17.2
Shear Modulus GV
52 GPa
Bulk Modulus KV
159 GPa
Shear Modulus GR
51 GPa
Bulk Modulus KR
159 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
159 GPa
Elastic Anisotropy
0.06
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LaBPt2 (mp-31052) 0.1337 0.000 3
NdBPt2 (mp-569341) 0.0666 0.000 3
CeBPt2 (mp-10468) 0.1289 0.016 3
LuBPt2 (mp-1095320) 0.0293 0.000 3
YbBPt2 (mp-1095422) 0.4732 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv B Pt
Final Energy/Atom
-7.3233 eV
Corrected Energy
-87.8800 eV
-87.8800 eV = -87.8800 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 156947
  • 156946
Submitted by
User remarks:
  • Yttrium platinum boride (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)