Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.266 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.430 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 150.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 280.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 120.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 200.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 172.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 280.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 120.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 123.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 320.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 320.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 160.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 120.1 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 285.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 258.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 258.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 280.3 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 285.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 320.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 200.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 80.1 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 200.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 258.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 285.2 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 285.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 120.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 280.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 86.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 247.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 280.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 160.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 258.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 240.2 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 160.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 172.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 258.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 120.1 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 150.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 280.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 160.2 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 280.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 320.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 200.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 200.2 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 280.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 280.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 172.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 285.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 160.2 |
BN (mp-984) | <1 1 1> | <0 1 0> | 160.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 95.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.02 | 0.00 | 0.00 |
0.00 | 1.99 | 0.00 |
0.00 | 0.00 | 2.03 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.68 | 0.00 | 0.00 |
0.00 | 3.48 | 0.00 |
0.00 | 0.00 | 3.69 |
Polycrystalline dielectric constant
εpoly∞
2.01
|
Polycrystalline dielectric constant
εpoly
3.61
|
Refractive Index n1.42 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.4768 | 0.003 | 3 |
AlPO4 (mp-5859) | 0.4194 | 0.011 | 3 |
AlPO4 (mp-37990) | 0.3998 | 0.014 | 3 |
AlPO4 (mp-557842) | 0.3841 | 0.011 | 3 |
AlPO4 (mp-675254) | 0.3863 | 0.012 | 3 |
CsAlSiO4 (mp-561457) | 0.7182 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5847 | 0.000 | 4 |
SiO2 (mp-559313) | 0.1300 | 0.009 | 2 |
SiO2 (mp-554543) | 0.1587 | 0.013 | 2 |
SiO2 (mp-7648) | 0.1491 | 0.007 | 2 |
SiO2 (mp-600029) | 0.1694 | 0.011 | 2 |
SiO2 (mp-560826) | 0.1420 | 0.012 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9046 eV |
Corrected Energy-150.7105 eV
-150.7105 eV = -142.2830 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)