Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.265 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.465 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 269.4 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 269.4 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 269.4 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 269.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 269.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 269.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 269.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 269.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 269.4 |
BN (mp-984) | <1 1 0> | <0 1 1> | 198.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 269.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 269.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 177.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 177.3 |
C (mp-66) | <1 1 1> | <0 1 0> | 89.8 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 269.4 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 269.4 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 269.4 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 269.4 |
C (mp-48) | <1 1 0> | <0 1 0> | 269.4 |
C (mp-48) | <1 1 1> | <0 1 0> | 269.4 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 269.4 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 269.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 0> | 89.8 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 269.4 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 269.4 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 269.4 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 269.4 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 269.4 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 89.8 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 269.4 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 0> | 89.8 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 269.4 |
ZnTe (mp-2176) | <1 1 1> | <0 1 0> | 269.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5859) | 0.3886 | 0.011 | 3 |
AlPO4 (mp-37990) | 0.3763 | 0.014 | 3 |
AlPO4 (mp-557362) | 0.4085 | 0.010 | 3 |
AlPO4 (mp-557842) | 0.3635 | 0.011 | 3 |
AlPO4 (mp-558056) | 0.3892 | 0.011 | 3 |
CsAlSiO4 (mp-561457) | 0.6967 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5707 | 0.000 | 4 |
SiO2 (mp-560527) | 0.1308 | 0.010 | 2 |
SiO2 (mp-600023) | 0.1837 | 0.014 | 2 |
CrN2 (mp-1096962) | 0.1743 | 0.370 | 2 |
CrN2 (mp-1096968) | 0.1652 | 0.360 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9030 eV |
Corrected Energy-401.8171 eV
-401.8171 eV = -379.3438 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)