Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.245 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.647 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2221 [20] |
HallC 2c 2 |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 199.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 156.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 199.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 199.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 199.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 186.1 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 156.5 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 156.5 |
CaCO3 (mp-3953) | <1 1 0> | <0 1 0> | 156.5 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 1> | 186.1 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 156.5 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 199.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.3886 | 0.012 | 3 |
AlPO4 (mp-557604) | 0.4248 | 0.010 | 3 |
AlPO4 (mp-557757) | 0.3983 | 0.015 | 3 |
AlPO4 (mp-683883) | 0.3970 | 0.018 | 3 |
Be(PO3)2 (mp-560521) | 0.3839 | 0.003 | 3 |
RbAlSiO4 (mp-6434) | 0.6038 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.5242 | 0.002 | 4 |
CsSi2HO5 (mp-557780) | 0.5821 | 0.005 | 4 |
KBePO4 (mp-7324) | 0.6081 | 0.000 | 4 |
KAlSi3O8 (mp-697670) | 0.6217 | 0.000 | 4 |
SiO2 (mp-639733) | 0.1737 | 0.018 | 2 |
SiO2 (mp-639480) | 0.1912 | 0.023 | 2 |
SiO2 (mp-557894) | 0.2366 | 0.016 | 2 |
CeSe2 (mp-1080632) | 0.2333 | 0.522 | 2 |
SiO2 (mp-644923) | 0.2369 | 0.011 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8837 eV |
Corrected Energy-400.8887 eV
-400.8887 eV = -378.4154 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)