Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.259 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.517 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 114.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 114.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 228.9 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 228.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 182.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 228.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 182.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 228.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 114.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 228.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 182.7 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 182.7 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 114.5 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 114.5 |
SiC (mp-8062) | <1 1 1> | <0 1 0> | 228.9 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 228.9 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 182.7 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 228.9 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 182.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.4695 | 0.012 | 3 |
AlPO4 (mp-557362) | 0.4974 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.4476 | 0.011 | 3 |
Be(PO3)2 (mp-560521) | 0.4467 | 0.003 | 3 |
AlPO4 (mp-1019510) | 0.4446 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.6244 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.6825 | 0.002 | 4 |
CsSi2HO5 (mp-557780) | 0.6439 | 0.005 | 4 |
KBePO4 (mp-7324) | 0.6567 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.6581 | 0.000 | 4 |
SiO2 (mp-600053) | 0.1660 | 0.017 | 2 |
SiO2 (mp-554267) | 0.1967 | 0.016 | 2 |
SiO2 (mp-560155) | 0.2028 | 0.020 | 2 |
SiO2 (mp-667383) | 0.1901 | 0.008 | 2 |
CeSe2 (mp-1080854) | 0.1944 | 0.522 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8972 eV |
Corrected Energy-803.0782 eV
-803.0782 eV = -758.1317 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)