Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.598 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.402 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH6C(NO)2 + HCNO + CoN + CoCO3 + N2 |
Band Gap2.800 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 120.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 120.9 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 125.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 161.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 169.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 282.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 120.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 117.4 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 201.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 282.0 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 124.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 161.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 201.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 241.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 117.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 322.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 117.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 161.2 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 201.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 80.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 322.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 201.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 201.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 234.7 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 169.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 118.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 161.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 322.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 201.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 282.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 201.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 282.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 120.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 322.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 80.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 248.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 234.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 234.7 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 161.2 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 174.3 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 201.5 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 282.0 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 201.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 161.2 |
C (mp-66) | <1 1 1> | <0 1 0> | 201.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 120.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 161.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 322.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 120.9 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 322.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H4WNCl6 (mp-780738) | 0.6984 | 0.000 | 4 |
MgH8(ClO6)2 (mp-989229) | 0.6203 | 0.009 | 4 |
FeH4C3O5 (mp-567010) | 0.5779 | 0.153 | 4 |
RuC4(O2F3)2 (mp-542700) | 0.6341 | 0.146 | 4 |
SbH4NCl6 (mp-849325) | 0.6557 | 0.000 | 4 |
ZnCoH18N6Cl5 (mp-706995) | 0.6467 | 0.000 | 5 |
NiH12C4(N2O3)2 (mp-600351) | 0.4312 | 0.476 | 5 |
MnH10S2(NO2)4 (mp-566172) | 0.5824 | 0.073 | 5 |
CoH16C4(NO)7 (mp-744418) | 0.6521 | 0.350 | 5 |
NiH12C4(N2O3)2 (mp-655099) | 0.4313 | 0.476 | 5 |
NiH44C12N8(ClO5)2 (mp-746343) | 0.6500 | 0.143 | 6 |
CoBH18Br2(N3F2)2 (mp-569520) | 0.6207 | 0.016 | 6 |
SnH24C6N2(OF3)2 (mp-698397) | 0.5494 | 0.077 | 6 |
LiCoH24C8(N2O3)4 (mp-600348) | 0.4355 | 0.457 | 6 |
LiH8C2S2NO5 (mp-605006) | 0.5967 | 0.196 | 6 |
NaAgH16C4S4(NO5)2 (mp-605018) | 0.6635 | 0.215 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co H C N O |
Final Energy/Atom-5.6003 eV |
Corrected Energy-440.6101 eV
-440.6101 eV = -425.6254 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)