Final Magnetic Moment2.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.516 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.485 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH6C(NO)2 + H5CNO3 + HCNO + Ni + C |
Band Gap2.150 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 333.0 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 200.6 |
Al (mp-134) | <1 1 0> | <1 0 0> | 333.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 137.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 224.9 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 299.9 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 75.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 75.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 299.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 266.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 224.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 333.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 199.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 333.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 333.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 333.0 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 137.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 150.0 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 333.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 224.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 224.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 266.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 230.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 230.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 333.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 299.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 75.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 266.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 224.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 333.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 199.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 199.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 333.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 199.8 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 224.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 299.9 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 75.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 266.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 266.4 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 266.4 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 266.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 133.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 299.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 75.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 299.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 333.0 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 200.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 75.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 1> | 200.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl2Cr3O12 (mp-560926) | 0.7245 | 0.000 | 3 |
H4WNCl6 (mp-780738) | 0.5904 | 0.000 | 4 |
MgH8(ClO6)2 (mp-989229) | 0.6095 | 0.012 | 4 |
FeH4C3O5 (mp-567010) | 0.6690 | 0.114 | 4 |
ZnP2(HO)4 (mp-697451) | 0.5625 | 0.083 | 4 |
SbH4NCl6 (mp-849325) | 0.5253 | 0.000 | 4 |
Mn2H8S3(NO6)2 (mp-762853) | 0.6445 | 0.001 | 5 |
LuP2H4NO7 (mp-601348) | 0.6491 | 0.000 | 5 |
CoH18C4N7O8 (mp-600278) | 0.4312 | 0.403 | 5 |
NiH12C4(N2O3)2 (mp-655099) | 0.0207 | 0.485 | 5 |
InPH4NO5 (mp-707924) | 0.6170 | 0.204 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.7128 | 0.119 | 6 |
NiH44C12N8(ClO5)2 (mp-746343) | 0.6853 | 0.147 | 6 |
SnH24C6N2(OF3)2 (mp-698397) | 0.7401 | 0.078 | 6 |
AsC4S2Cl2O2F13 (mp-560424) | 0.6810 | 0.226 | 6 |
LiCoH24C8(N2O3)4 (mp-600348) | 0.1705 | 0.457 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv H C N O |
Final Energy/Atom-5.5752 eV |
Corrected Energy-313.8144 eV
-313.8144 eV = -301.0589 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)