Final Magnetic Moment4.029 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.688 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + H2O + FeBr2 + H4BrN + C |
Band Gap3.800 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BN (mp-984) | <0 0 1> | <0 0 1> | 65.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 196.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 131.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 148.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 262.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 328.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 328.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 262.4 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 149.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 328.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 196.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 328.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 328.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 328.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 328.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 149.9 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 163.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 328.0 |
C (mp-66) | <1 1 0> | <1 0 1> | 163.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 328.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 328.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 328.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 328.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 262.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 262.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 328.0 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 328.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 149.9 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 133.5 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 328.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 262.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 328.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 163.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 328.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 196.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 262.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 328.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 131.2 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 133.5 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 262.4 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 262.4 |
Si (mp-149) | <1 1 0> | <0 0 1> | 328.0 |
Au (mp-81) | <1 1 0> | <0 0 1> | 196.8 |
CdSe (mp-2691) | <1 1 0> | <1 0 1> | 163.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 133.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 65.6 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 262.4 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 262.4 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 328.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg4Al3(HO)17 (mp-690136) | 0.7440 | 0.057 | 4 |
CoH12(ClO3)2 (mp-743756) | 0.6188 | 0.007 | 4 |
Na5P5(H9O7)2 (mp-706715) | 0.7216 | 0.016 | 4 |
NiH12(ClO3)2 (mp-25107) | 0.6972 | 0.014 | 4 |
CoH12(BrO3)2 (mp-542452) | 0.6442 | 0.000 | 4 |
Na4GeH28(Se2O7)2 (mp-721293) | 0.6414 | 0.020 | 5 |
FePH5CO4 (mp-601661) | 0.6344 | 0.030 | 5 |
MnH8C2NCl3 (mp-567451) | 0.6172 | 0.194 | 5 |
CdH8C2Br3N (mp-600182) | 0.6340 | 0.065 | 5 |
CuH8C2NCl3 (mp-698413) | 0.6397 | 0.059 | 5 |
CoH14C3NCl3O2 (mp-600527) | 0.2880 | 0.089 | 6 |
NiH14C3NCl3O2 (mp-600519) | 0.2687 | 0.090 | 6 |
MnH14C3NCl3O2 (mp-600501) | 0.3141 | 0.181 | 6 |
MnH10CNCl3O2 (mp-600507) | 0.4642 | 0.172 | 6 |
MnH12C2NCl3O2 (mp-743974) | 0.5027 | 0.184 | 6 |
H24RuC7S3NCl3O4 (mp-738597) | 0.6533 | 0.206 | 7 |
NaAgH16C4S4(NO5)2 (mp-605018) | 0.6942 | 0.215 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv H C Br N O |
Final Energy/Atom-4.8596 eV |
Corrected Energy-483.0756 eV
-483.0756 eV = -466.5253 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)