Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.922 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoH18CN6ClO3 + H5CNO3 + H6C(NO)2 + H4NCl + CoO + Co |
Band Gap0.655 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 279.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 279.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 159.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 175.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 279.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 175.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 279.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 196.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 175.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 175.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 148.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 93.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 148.2 |
BN (mp-984) | <0 0 1> | <1 0 1> | 175.0 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 129.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 279.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 279.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 175.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 279.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 93.0 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 279.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 148.2 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 175.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 279.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 159.6 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 1> | 175.0 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 93.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 148.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 279.0 |
Au (mp-81) | <1 1 0> | <1 0 0> | 148.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 279.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 279.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 259.4 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 279.0 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 279.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 0 0> | 148.2 |
CaCO3 (mp-3953) | <1 1 0> | <0 1 1> | 159.6 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 186.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 279.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 279.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 279.0 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 1> | 175.0 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 279.0 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 93.0 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 279.0 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 279.0 |
MgF2 (mp-1249) | <0 0 1> | <1 1 0> | 196.9 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 129.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoH14N5O9 (mp-744996) | 0.6094 | 0.185 | 4 |
CoH22C3(N3O4)2 (mp-746670) | 0.6676 | 0.029 | 5 |
CoH19S3N5O11 (mp-745100) | 0.6495 | 0.077 | 5 |
CoH16C3N8O7 (mp-744002) | 0.6959 | 0.120 | 5 |
H22RhC3(N3O4)2 (mp-600156) | 0.6901 | 0.023 | 5 |
H22IrC3(N3O4)2 (mp-698362) | 0.6629 | 0.029 | 5 |
PuCoH24C4N6O13 (mp-744896) | 0.6484 | 0.060 | 6 |
MnH9CNCl3O2 (mp-743948) | 0.7429 | 0.160 | 6 |
ReH22C4S4N8Cl8O3 (mp-707926) | 0.7368 | 0.080 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co H C N Cl O |
Final Energy/Atom-5.3316 eV |
Corrected Energy-810.6175 eV
-810.6175 eV = -789.0757 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)