material

Ba2LiN

ID:

mp-605860

DOI:

10.17188/1277484


Tags: Lithium dibarium nitride

Material Details

Final Magnetic Moment
0.594 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.365 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.055 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Li3N + Ba3N
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P42/nmc [137]
Hall
P 4n 2n 1n
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 245651 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.000 136.7
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.000 273.5
GaP (mp-2490) <1 0 0> <0 0 1> 0.001 273.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.004 273.5
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.007 181.3
Mg (mp-153) <1 1 1> <0 0 1> 0.008 273.5
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.010 256.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.017 136.7
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.018 273.5
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.021 273.5
Ag (mp-124) <1 1 0> <1 0 1> 0.025 145.3
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.025 256.4
GdScO3 (mp-5690) <0 0 1> <1 1 1> 0.025 193.7
Ag (mp-124) <1 0 0> <0 0 1> 0.030 68.4
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.036 136.7
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.036 128.2
Al (mp-134) <1 0 0> <0 0 1> 0.036 273.5
Mg (mp-153) <1 0 1> <0 0 1> 0.037 205.1
GaN (mp-804) <1 1 1> <0 0 1> 0.044 273.5
Si (mp-149) <1 0 0> <0 0 1> 0.046 273.5
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.049 273.5
TeO2 (mp-2125) <0 0 1> <1 1 1> 0.053 193.7
MoSe2 (mp-1634) <1 1 0> <1 1 0> 0.058 181.3
Au (mp-81) <1 0 0> <0 0 1> 0.060 68.4
Mg (mp-153) <1 1 0> <1 0 0> 0.068 256.4
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.075 273.5
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.082 256.4
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.097 128.2
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.100 273.5
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.103 68.4
CdS (mp-672) <1 0 1> <1 0 0> 0.104 128.2
GaN (mp-804) <1 0 1> <0 0 1> 0.104 205.1
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.113 256.4
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.120 256.4
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.129 273.5
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.132 181.3
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.143 256.4
Ge (mp-32) <1 0 0> <0 0 1> 0.150 68.4
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.159 128.2
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.170 256.4
ZnO (mp-2133) <1 1 0> <1 1 0> 0.172 181.3
GaAs (mp-2534) <1 0 0> <0 0 1> 0.199 68.4
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.232 68.4
InP (mp-20351) <1 0 0> <0 0 1> 0.267 68.4
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.278 136.7
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.297 273.5
WSe2 (mp-1821) <1 1 0> <1 1 0> 0.331 181.3
TeO2 (mp-2125) <1 1 0> <0 0 1> 0.334 205.1
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.371 273.5
SiC (mp-7631) <1 1 1> <1 0 0> 0.403 256.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
32 3 11 0 0 0
3 32 11 0 0 0
11 11 25 0 0 0
0 0 0 5 0 0
0 0 0 0 5 0
0 0 0 0 0 3
Compliance Tensor Sij (10-12Pa-1)
36.6 2.1 -17.3 0 0 0
2.1 36.6 -17.3 0 0 0
-17.3 -17.3 55.4 0 0 0
0 0 0 190.1 0 0
0 0 0 0 190.1 0
0 0 0 0 0 344.6
Shear Modulus GV
7 GPa
Bulk Modulus KV
16 GPa
Shear Modulus GR
5 GPa
Bulk Modulus KR
16 GPa
Shear Modulus GVRH
6 GPa
Bulk Modulus KVRH
16 GPa
Elastic Anisotropy
1.54
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
VOF3 (mp-764398) 0.6907 0.058 3
Zr2TeBr12 (mp-28672) 0.6695 0.000 3
Ti2SCl12 (mp-649080) 0.5861 0.016 3
FeH2Cl5O3 (mp-735518) 0.6408 0.792 4
FeH8(ClO2)2 (mp-743178) 0.6817 0.050 4
TeMoCl7O (mp-617022) 0.7273 0.034 4
FeO3 (mp-863847) 0.6219 0.540 2
TeI4 (mp-567269) 0.5165 0.002 2
Cs11O3 (mp-562001) 0.6284 0.004 2
TeI4 (mp-651155) 0.5176 0.002 2
TeI4 (mp-570884) 0.5566 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Li_sv N
Final Energy/Atom
-3.7952 eV
Corrected Energy
-124.3343 eV
Uncorrected energy = -121.4463 eV Composition-based energy adjustment (-0.361 eV/atom x 8.0 atoms) = -2.8880 eV Corrected energy = -124.3343 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 245651
Submitted by
User remarks:
  • Lithium dibarium nitride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)