Final Magnetic Moment13.018 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.440 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.440 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNp + In |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 109.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 267.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 296.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 181.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 125.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 118.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 89.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 326.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 237.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 89.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 314.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 326.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 42.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 59.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 167.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 188.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 36.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 89.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 188.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 104.9 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 207.8 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 181.7 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 145.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 356.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 83.9 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 209.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 181.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 89.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 326.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 254.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 356.8 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 207.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 83.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 89.0 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 109.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 167.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 89.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 89.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 109.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 293.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 237.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 42.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 59.4 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 109.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 293.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 89.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 326.5 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 207.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 104.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 267.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1119 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0484 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.0011 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.0404 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.0149 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2148 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3601 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4013 | 0.193 | 4 |
LaNp3 (mp-981435) | 0.0005 | 0.706 | 2 |
TmPa3 (mp-978994) | 0.0006 | 0.163 | 2 |
LaBi3 (mp-867248) | 0.0006 | 0.000 | 2 |
Zr3Cu (mp-580287) | 0.0007 | 0.132 | 2 |
MgZr (mp-1094974) | 0.0007 | 0.087 | 2 |
P (mp-674158) | 0.0011 | 3.518 | 1 |
Xe (mp-611517) | 0.0011 | 0.006 | 1 |
Eu (mp-623532) | 0.0011 | 0.035 | 1 |
He (mp-614456) | 0.0011 | 0.008 | 1 |
Au (mp-81) | 0.0011 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Np In_d |
Final Energy/Atom-9.9584 eV |
Corrected Energy-39.8337 eV
-39.8337 eV = -39.8337 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)