@article{YuRon2007, author = "Rong, Yu and Qian, Zhan and L.C., De Jonghe", title = "Crystal Structures of and Displacive Transitions in OsN2, IrN2, RuN2, and RhN2", journal = "Angewandte Chemie. International Edition", year = "2007", volume = "46", pages = "1136-1140", ASTM_id = "ACIEF5" }