Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.424 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrInAu2 + PrIn3 + In2Au |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 177.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 320.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 248.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 320.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 355.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 106.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 177.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 320.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 320.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 284.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 269.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 284.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 269.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 248.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 177.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 142.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 320.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 320.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 289.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 248.9 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 248.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 177.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 320.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 355.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 284.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 142.2 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 193.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 355.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 248.9 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 142.2 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 248.9 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 289.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 248.9 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 248.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 320.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 177.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 71.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 106.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 248.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 320.0 |
C (mp-66) | <1 1 0> | <0 1 1> | 289.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 320.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 284.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 320.0 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 284.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 284.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 179.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 284.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 142.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce(In2Pd)2 (mp-641911) | 0.3238 | 0.002 | 3 |
Nd(In2Au)2 (mp-607126) | 0.0803 | 0.010 | 3 |
La(In2Au)2 (mp-21523) | 0.1877 | 0.000 | 3 |
Yb2Sn5Pt3 (mp-21820) | 0.4860 | 0.000 | 3 |
Ce(In2Au)2 (mp-21537) | 0.1340 | 0.016 | 3 |
K2BaCdSb2 (mp-863761) | 0.7282 | 0.000 | 4 |
K2SrCdSb2 (mp-863758) | 0.6642 | 0.000 | 4 |
Mg2Si3 (mp-1073201) | 0.6813 | 0.253 | 2 |
MgSi2 (mp-1073396) | 0.6917 | 0.197 | 2 |
Mg3Si4 (mp-1075018) | 0.6976 | 0.223 | 2 |
Mg3Si4 (mp-1075397) | 0.6671 | 0.335 | 2 |
Mg6Si5 (mp-1073934) | 0.6976 | 0.199 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 In_d Au |
Final Energy/Atom-3.6145 eV |
Corrected Energy-101.2056 eV
-101.2056 eV = -101.2056 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)