material

TiCo3

ID:

mp-608

DOI:

10.17188/1277595


Tags: Cobalt titanium (3/1)

Material Details

Final Magnetic Moment
2.699 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-0.259 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.95 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 97992 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.001 65.1
GaP (mp-2490) <1 1 1> <1 1 1> 0.002 157.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.004 157.8
Ag (mp-124) <1 1 0> <1 1 0> 0.004 73.6
Ag (mp-124) <1 1 1> <1 1 1> 0.004 90.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.006 325.3
Al (mp-134) <1 0 0> <1 0 0> 0.007 65.1
Au (mp-81) <1 1 0> <1 1 0> 0.007 73.6
Au (mp-81) <1 1 1> <1 1 1> 0.007 90.1
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.009 208.2
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.012 52.0
NaCl (mp-22862) <1 0 0> <1 0 0> 0.013 65.1
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.019 128.8
Cu (mp-30) <1 0 0> <1 0 0> 0.020 13.0
Cu (mp-30) <1 1 0> <1 1 0> 0.022 18.4
Cu (mp-30) <1 1 1> <1 1 1> 0.023 22.5
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.029 325.3
AlN (mp-661) <1 0 1> <1 0 0> 0.032 195.2
CdS (mp-672) <1 0 0> <1 1 0> 0.035 202.4
PbSe (mp-2201) <1 1 0> <1 1 0> 0.037 55.2
PbSe (mp-2201) <1 1 1> <1 1 1> 0.038 67.6
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.048 67.6
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.049 67.6
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.054 195.2
GaSe (mp-1943) <1 0 0> <1 0 0> 0.055 273.2
CdS (mp-672) <1 1 1> <1 0 0> 0.059 52.0
ZnO (mp-2133) <1 1 0> <1 1 0> 0.067 331.2
GaSb (mp-1156) <1 1 0> <1 1 0> 0.070 55.2
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.072 202.4
GaSb (mp-1156) <1 1 1> <1 1 1> 0.072 67.6
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.072 325.3
TiO2 (mp-390) <0 0 1> <1 0 0> 0.082 117.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.087 55.2
CdWO4 (mp-19387) <0 1 0> <1 1 1> 0.087 293.0
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.102 165.6
CdSe (mp-2691) <1 1 0> <1 1 0> 0.104 55.2
CdSe (mp-2691) <1 1 1> <1 1 1> 0.107 67.6
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.107 55.2
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.110 67.6
LaF3 (mp-905) <1 0 1> <1 0 0> 0.122 208.2
Te2W (mp-22693) <0 1 0> <1 1 1> 0.124 270.4
Fe2O3 (mp-24972) <1 0 1> <1 0 0> 0.126 221.2
SiC (mp-11714) <1 1 0> <1 1 1> 0.127 270.4
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.127 325.3
Te2W (mp-22693) <1 1 0> <1 1 0> 0.131 110.4
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.134 55.2
CaCO3 (mp-3953) <1 0 1> <1 0 0> 0.138 91.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.144 65.1
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.147 65.1
SiC (mp-11714) <1 0 0> <1 0 0> 0.155 156.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
258 162 162 0 0 0
162 258 162 0 0 0
162 162 258 0 0 0
0 0 0 119 0 0
0 0 0 0 119 0
0 0 0 0 0 119
Compliance Tensor Sij (10-12Pa-1)
7.5 -2.9 -2.9 0 0 0
-2.9 7.5 -2.9 0 0 0
-2.9 -2.9 7.5 0 0 0
0 0 0 8.4 0 0
0 0 0 0 8.4 0
0 0 0 0 0 8.4
Shear Modulus GV
91 GPa
Bulk Modulus KV
194 GPa
Shear Modulus GR
75 GPa
Bulk Modulus KR
194 GPa
Shear Modulus GVRH
83 GPa
Bulk Modulus KVRH
194 GPa
Elastic Anisotropy
1.05
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.000 3
LiCa6Ge (mp-12609) 0.0000 0.180 3
GaFeNi2 (mp-1065359) 0.0412 0.066 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.118 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
Be3Tc (mp-977552) 0.0000 0.000 2
AlC3 (mp-1065540) 0.0000 2.748 2
TiOs3 (mp-980203) 0.0000 0.222 2
DyPt3 (mp-2465) 0.0000 0.000 2
MgCd3 (mp-1094839) 0.0000 0.015 2
Sr (mp-76) 0.0000 0.006 1
N2 (mp-1056857) 0.0000 0.000 1
Ni (mp-1056486) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.001 1
Pd (mp-1056438) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Co
Final Energy/Atom
-7.5641 eV
Corrected Energy
-30.2562 eV
Uncorrected energy = -30.2562 eV Corrected energy = -30.2562 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 97992
  • 187964
  • 625484
  • 625468
  • 625462
  • 102708
  • 97993
  • 625481
  • 187984
Submitted by
User remarks:
  • Cobalt titanium (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)