Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.963 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP31c [163] |
Hall-P 3 2c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.7 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 111.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 367.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 298.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 137.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 304.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 167.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 272.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 50.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 321.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 203.2 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 278.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 23.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 137.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 160.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 206.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 176.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 264.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 203.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 206.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 206.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 254.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 367.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 367.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 91.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 298.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 223.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 223.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 91.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 152.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 203.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 206.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 137.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 278.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 275.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(SbO3)2 (mp-9125) | 0.2430 | 0.000 | 3 |
Li2MnF6 (mp-777332) | 0.2474 | 0.014 | 3 |
Mn(AsO3)2 (mp-19409) | 0.2276 | 0.000 | 3 |
CaTi2O6 (mp-1079825) | 0.2203 | 0.182 | 3 |
Li2MnF6 (mp-765003) | 0.2187 | 0.000 | 3 |
LiCaCrF6 (mp-565468) | 0.0616 | 0.000 | 4 |
LiCdCoF6 (mp-566148) | 0.0871 | 0.001 | 4 |
LiCaGaF6 (mp-12829) | 0.0181 | 0.000 | 4 |
LiCaCoF6 (mp-555529) | 0.0449 | 0.000 | 4 |
LiCaNiF6 (mp-608204) | 0.0392 | 0.000 | 4 |
Rb2O (mp-755459) | 0.4229 | 0.018 | 2 |
CaCl2 (mp-571642) | 0.4144 | 0.001 | 2 |
SiO2 (mp-10948) | 0.4035 | 0.254 | 2 |
SiO2 (mp-32667) | 0.4201 | 0.241 | 2 |
Co2N (mp-22631) | 0.4258 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ca_sv Ni_pv F |
Final Energy/Atom-4.7469 eV |
Corrected Energy-89.7719 eV
-89.7719 eV = -85.4439 eV (uncorrected energy) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)