NaNiF3

ID:

mp-561480

DOI:

10.17188/1272095


Tags: Sodium nickel fluoride High pressure experimental phase Sodium trifluoroniccolate Sodium nickel trifluoride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.404 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.126 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NaNiF3
Band Gap
4.611 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 9008 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.000 151.6
TeO2 (mp-2125) <0 1 1> <0 0 1> 0.002 151.6
GaP (mp-2490) <1 1 1> <0 1 0> 0.005 210.3
CaF2 (mp-2741) <1 1 1> <0 1 0> 0.007 210.3
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.008 203.0
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.015 121.2
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.017 43.5
TiO2 (mp-2657) <1 1 0> <0 1 1> 0.018 155.5
AlN (mp-661) <0 0 1> <0 0 1> 0.019 151.6
YVO4 (mp-19133) <1 0 1> <0 1 1> 0.020 207.4
WS2 (mp-224) <1 0 0> <1 1 1> 0.025 135.3
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.026 53.0
BN (mp-984) <1 1 0> <0 1 0> 0.028 168.2
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.028 53.0
BN (mp-984) <1 1 1> <0 1 0> 0.030 168.2
Te2W (mp-22693) <0 0 1> <0 0 1> 0.031 333.4
ZnO (mp-2133) <1 0 1> <1 0 0> 0.033 217.5
InAs (mp-20305) <1 0 0> <1 1 0> 0.036 302.5
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.036 84.1
CeO2 (mp-20194) <1 1 0> <0 1 0> 0.038 42.1
BaF2 (mp-1029) <1 1 0> <0 1 0> 0.038 168.2
NdGaO3 (mp-3196) <1 1 0> <1 1 0> 0.040 60.5
Si (mp-149) <1 1 0> <0 1 0> 0.040 42.1
ZnTe (mp-2176) <1 0 0> <1 1 0> 0.043 302.5
NdGaO3 (mp-3196) <1 1 1> <1 1 1> 0.044 67.7
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.046 333.4
SiC (mp-11714) <1 1 1> <0 0 1> 0.052 333.4
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.052 304.5
BN (mp-984) <0 0 1> <0 1 1> 0.059 103.7
Si (mp-149) <1 1 1> <0 1 0> 0.066 210.3
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.066 30.3
Cu (mp-30) <1 1 0> <0 1 0> 0.067 168.2
Te2W (mp-22693) <0 1 0> <1 1 1> 0.067 270.7
NdGaO3 (mp-3196) <0 1 1> <0 1 1> 0.069 51.8
SiC (mp-7631) <1 0 1> <1 1 0> 0.070 242.0
CeO2 (mp-20194) <1 1 1> <0 1 0> 0.070 210.3
NdGaO3 (mp-3196) <0 1 0> <0 1 0> 0.071 42.1
SiC (mp-7631) <0 0 1> <0 0 1> 0.073 151.6
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.074 168.2
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.074 304.5
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.075 304.5
C (mp-48) <0 0 1> <0 0 1> 0.076 181.9
LaF3 (mp-905) <0 0 1> <1 0 1> 0.078 318.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.079 151.6
Ga2O3 (mp-886) <1 0 -1> <1 1 0> 0.080 302.5
WS2 (mp-224) <0 0 1> <1 0 1> 0.081 53.0
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.081 53.0
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.086 130.5
InSb (mp-20012) <1 1 0> <0 1 0> 0.091 126.2
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.091 304.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
132 45 59 0 0 0
45 129 42 0 0 0
59 42 113 0 0 0
0 0 0 30 0 0
0 0 0 0 41 0
0 0 0 0 0 36
Compliance Tensor Sij (10-12Pa-1)
10.3 -2.1 -4.6 0 0 0
-2.1 9.2 -2.3 0 0 0
-4.6 -2.3 12 0 0 0
0 0 0 33.2 0 0
0 0 0 0 24.2 0
0 0 0 0 0 28.2
Shear Modulus GV
37 GPa
Bulk Modulus KV
74 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
74 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
74 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.29

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.25 0.00 0.00
0.00 2.25 0.00
0.00 0.00 2.24
Dielectric Tensor εij (total)
6.23 0.00 0.00
0.00 9.21 0.00
0.00 0.00 6.09
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.25
Polycrystalline dielectric constant εpoly
(total)
7.18
Refractive Index n
1.50
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaNiF3 (mp-608590) 0.0376 0.126 3
NaZnF3 (mp-3795) 0.0569 0.000 3
MgSiO3 (mp-3547) 0.0615 0.215 3
NaCoF3 (mp-555201) 0.0635 0.166 3
GdCrO3 (mp-19598) 0.0504 0.000 3
Sm2MgIrO6 (mp-980108) 0.1376 0.006 4
Ca2FeIrO6 (mvc-5784) 0.1526 0.000 4
Ca2SnIrO6 (mvc-5666) 0.0900 0.067 4
Ca2SnSbO6 (mvc-3972) 0.1130 0.076 4
Ca2CoIrO6 (mvc-5820) 0.1593 0.000 4
U2S3 (mp-672690) 0.6843 0.194 2
Al2O3 (mp-642363) 0.6119 0.280 2
Cr3C2 (mp-570112) 0.6440 0.030 2
Ga2O3 (mp-13134) 0.6949 0.284 2
Fe2O3 (mp-1078361) 0.6846 0.704 2
LiLaNdSbO6 (mp-776091) 0.2368 0.006 5
CaLaCrMoO6 (mvc-9974) 0.2935 0.010 5
CaLaCrSnO6 (mvc-9999) 0.2891 0.036 5
LaMgCrSnO6 (mvc-9925) 0.2927 0.148 5
CaLaMnRuO6 (mp-690556) 0.2643 0.080 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
700 eV
# of K-points
None
U Values
Ni: 6.2 eV
Pseudopotentials
VASP PAW: Na_pv Ni_pv F
Final Energy/Atom
-4.2423 eV
Corrected Energy
-93.5017 eV
-93.5017 eV = -84.8457 eV (uncorrected energy) - 8.6560 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 9008
  • 200062
  • 25533
  • 192142
  • 192144
  • 72319
  • 192140
Submitted by
User remarks:
  • Sodium trifluoroniccolate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)