Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.903 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.168 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg3O4 + MnO2 + O2 |
Band Gap0.766 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 255.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 241.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 236.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 282.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 94.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 282.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 94.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 236.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 282.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 142.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 186.7 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 290.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 282.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 217.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 236.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 322.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 150.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 161.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 236.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 322.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 142.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 225.1 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 282.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 145.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 189.5 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 322.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 94.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 301.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 331.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 236.9 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 217.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 94.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 284.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 331.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 331.7 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 301.4 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 60.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 225.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 300.1 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 241.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 47.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 236.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 331.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 180.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 311.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 300.1 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 180.8 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 282.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 -1> | 217.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgBrO4 (mp-756139) | 0.0904 | 0.038 | 3 |
NaMnO4 (mp-765753) | 0.0971 | 0.059 | 3 |
CrAgO4 (mp-850137) | 0.3280 | 0.030 | 3 |
USeO6 (mp-562338) | 0.5892 | 0.000 | 3 |
CrHgO4 (mp-19155) | 0.5825 | 0.004 | 3 |
Cd2BiAsO6 (mp-556653) | 0.5823 | 0.000 | 4 |
LiCoPO4 (mp-765449) | 0.6230 | 0.082 | 4 |
LiFePO4 (mp-761476) | 0.6060 | 0.063 | 4 |
Ca2BiAsO6 (mvc-16445) | 0.5578 | 0.000 | 4 |
Ca2VBiO6 (mvc-16459) | 0.5776 | 0.000 | 4 |
K2USO7F2 (mp-863004) | 0.7477 | 0.185 | 5 |
SrCaP2WO8 (mvc-3024) | 0.7039 | 0.266 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Ag O |
Final Energy/Atom-5.4524 eV |
Corrected Energy-148.5213 eV
Uncorrected energy = -130.8573 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.668 eV/atom x 4.0 atoms) = -6.6720 eV
Corrected energy = -148.5213 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)