Final Magnetic Moment3.033 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.947 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom2.242 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 213.1 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 236.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 74.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 115.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 144.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 109.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 109.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 236.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 207.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 306.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 201.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 190.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 115.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 132.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 115.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 155.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 121.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 178.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 240.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 109.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 178.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 190.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 161.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 236.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 115.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 161.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 334.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 201.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 190.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 339.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 132.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 155.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 121.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 207.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 109.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 184.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 109.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 247.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 282.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 311.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 270.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 138.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 201.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 97.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 201.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 311.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 132.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H3Pt (mp-977343) | 0.7341 | 0.387 | 2 |
HfPd5 (mp-1077225) | 0.4389 | 1.571 | 2 |
CeSe2 (mp-1080319) | 0.0554 | 2.385 | 2 |
Hg (mp-611219) | 0.1465 | 0.084 | 1 |
B (mp-1055985) | 0.4978 | 0.708 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: V_pv S |
Final Energy/Atom-4.3946 eV |
Corrected Energy-14.5107 eV
-14.5107 eV = -13.1838 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)