material

Fe(BW)2

ID:

mp-613327

DOI:

10.17188/1277742


Tags: Tungsten iron boride (2/1/2) - HT

Material Details

Final Magnetic Moment
0.043 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.329 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.098 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.12 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Fe(BW)2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mbm [127]
Hall
-P 4 2ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 43016 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <0 0 1> 0.000 32.4
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.000 291.4
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.010 92.0
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.014 32.4
Al (mp-134) <1 1 0> <1 0 0> 0.018 92.0
NaCl (mp-22862) <1 1 0> <1 0 0> 0.030 92.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.049 129.5
MgO (mp-1265) <1 0 0> <0 0 1> 0.057 161.9
Al (mp-134) <1 0 0> <0 0 1> 0.064 32.4
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.081 259.1
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.104 64.8
Cu (mp-30) <1 0 0> <0 0 1> 0.107 64.8
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.108 124.6
BN (mp-984) <0 0 1> <1 0 0> 0.110 147.2
C (mp-48) <0 0 1> <1 0 0> 0.111 36.8
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.123 331.3
KCl (mp-23193) <1 0 0> <0 0 1> 0.124 161.9
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.127 55.2
AlN (mp-661) <1 0 1> <0 0 1> 0.128 194.3
SiC (mp-11714) <1 1 1> <1 1 1> 0.132 166.2
PbS (mp-21276) <1 0 0> <0 0 1> 0.133 291.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.134 32.4
Ni (mp-23) <1 0 0> <0 0 1> 0.163 161.9
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.169 260.7
Mg (mp-153) <1 1 0> <1 0 0> 0.173 257.6
Ga2O3 (mp-886) <1 1 0> <0 0 1> 0.186 291.4
LiTaO3 (mp-3666) <0 0 1> <1 1 0> 0.192 234.2
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.198 92.0
CdS (mp-672) <1 1 1> <0 0 1> 0.206 259.1
C (mp-66) <1 0 0> <0 0 1> 0.210 64.8
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.211 276.0
MoS2 (mp-1434) <1 0 1> <1 0 0> 0.216 276.0
SiO2 (mp-6930) <1 1 0> <1 1 1> 0.219 332.4
LaF3 (mp-905) <1 1 1> <1 1 1> 0.222 207.7
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.224 92.0
LiTaO3 (mp-3666) <1 0 0> <1 1 1> 0.227 290.8
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.229 92.0
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.229 257.6
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.243 55.2
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.252 312.3
BN (mp-984) <1 0 0> <0 0 1> 0.273 97.1
LiNbO3 (mp-3731) <0 0 1> <1 1 0> 0.280 234.2
BN (mp-984) <1 1 1> <1 1 0> 0.303 234.2
InAs (mp-20305) <1 1 1> <1 0 1> 0.307 260.7
WS2 (mp-224) <1 0 0> <1 0 0> 0.326 92.0
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.327 92.0
GaAs (mp-2534) <1 1 0> <1 0 0> 0.328 92.0
Ni (mp-23) <1 1 1> <1 0 0> 0.329 147.2
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.332 32.4
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.337 92.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
496 243 243 0 0 0
243 482 218 0 0 0
243 218 482 0 0 0
0 0 0 179 0 0
0 0 0 0 242 0
0 0 0 0 0 242
Compliance Tensor Sij (10-12Pa-1)
3.1 -1.1 -1.1 0 0 0
-1.1 3 -0.8 0 0 0
-1.1 -0.8 3 0 0 0
0 0 0 5.6 0 0
0 0 0 0 4.1 0
0 0 0 0 0 4.1
Shear Modulus GV
183 GPa
Bulk Modulus KV
319 GPa
Shear Modulus GR
168 GPa
Bulk Modulus KR
318 GPa
Shear Modulus GVRH
175 GPa
Bulk Modulus KVRH
319 GPa
Elastic Anisotropy
0.45
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li(YSi)2 (mp-7350) 0.1638 0.047 3
La2InGe2 (mp-21288) 0.1015 0.000 3
Pr2InGe2 (mp-20715) 0.1418 0.000 3
Nd2InGe2 (mp-20575) 0.1423 0.000 3
Li(NdSi)2 (mp-1091362) 0.0916 0.014 3
Pr3Si2 (mp-1079937) 0.2817 0.000 2
La3Si2 (mp-10162) 0.2521 0.005 2
Np3Si2 (mp-1079895) 0.2866 0.438 2
Pu3Si2 (mp-1080146) 0.1257 0.000 2
Ce3Si2 (mp-1079007) 0.2228 0.001 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Fe_pv B W_pv
Final Energy/Atom
-9.8779 eV
Corrected Energy
-98.7792 eV
-98.7792 eV = -98.7792 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43016
Submitted by
User remarks:
  • Tungsten iron boride (2/1/2) - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)