Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.929 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMo8O23 + Tl2Mo4O13 + MoO2 |
Band Gap0.977 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 309.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 309.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 121.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 129.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 154.9 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 258.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 206.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 129.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 133.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 121.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 129.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 309.8 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 258.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 258.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 258.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 309.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 -1> | 164.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 202.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 154.9 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 258.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 103.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 103.3 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 129.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 103.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 258.1 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 258.1 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 309.8 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 206.5 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 309.8 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 242.0 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 242.0 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 242.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 258.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 154.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 309.8 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 129.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 309.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 -1> | 129.3 |
Mg (mp-153) | <1 1 0> | <1 0 -1> | 258.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 227.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 121.0 |
GaP (mp-2490) | <1 1 0> | <1 0 -1> | 129.3 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 -1> | 129.3 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 309.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 -1> | 129.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 309.8 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 258.1 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 309.8 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 -1> | 129.3 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 133.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaV2O6 (mvc-11947) | 0.7010 | 0.131 | 3 |
Hg2Mo2O7 (mp-704753) | 0.5865 | 0.003 | 3 |
Cs(MoO3)3 (mp-541213) | 0.2379 | 0.046 | 3 |
K(MoO3)3 (mp-19607) | 0.1371 | 0.039 | 3 |
Tl(MoO3)3 (mp-615697) | 0.0191 | 0.038 | 3 |
Rb2Nb3Cl7O5 (mp-558393) | 0.7295 | 0.000 | 4 |
Tl2OsCBr2OF3 (mp-556622) | 0.6928 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Tl_d Mo_pv O |
Final Energy/Atom-6.7379 eV |
Corrected Energy-206.7634 eV
Uncorrected energy = -175.1854 eV
Composition-based energy adjustment (-0.687 eV/atom x 18.0 atoms) = -12.3660 eV
Composition-based energy adjustment (-3.202 eV/atom x 6.0 atoms) = -19.2120 eV
Corrected energy = -206.7634 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)