Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.616 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.239 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmmn [59] |
HallP 2 2ab 1ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 246.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 96.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 289.7 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 219.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 128.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 128.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 146.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 225.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 219.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 151.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 219.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 289.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 226.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 128.8 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 146.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 151.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 257.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 257.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 164.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 219.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 289.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 302.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 289.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 75.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 225.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 289.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 161.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 219.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 354.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 219.1 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 196.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 161.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 246.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 257.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 100.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 161.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 321.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 289.7 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 196.6 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 246.4 |
GaSe (mp-1943) | <1 1 0> | <1 0 1> | 246.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 289.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 257.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 327.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 321.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 196.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 96.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 73.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na(NiO2)2 (mp-764934) | 0.2295 | 0.002 | 3 |
SrCr2O4 (mp-562321) | 0.2739 | 0.000 | 3 |
Na(CoO2)2 (mp-510559) | 0.1458 | 0.039 | 3 |
SrCr2O4 (mp-647134) | 0.2743 | 0.000 | 3 |
BaCr2O4 (mp-615701) | 0.0065 | 0.000 | 3 |
LiMn3(O2F)2 (mp-767123) | 0.5484 | 0.093 | 4 |
NaTiFeO4 (mp-648745) | 0.5793 | 0.214 | 4 |
Li2V(OF)2 (mp-764705) | 0.5863 | 0.215 | 4 |
Mg2AgWO6 (mvc-5923) | 0.5756 | 0.088 | 4 |
Li2VOF3 (mp-767622) | 0.5518 | 0.092 | 4 |
Pb3O4 (mp-636813) | 0.5301 | 0.038 | 2 |
U2S3 (mp-672690) | 0.6468 | 0.194 | 2 |
Sr4N3 (mp-685023) | 0.6604 | 0.191 | 2 |
Yb2S3 (mp-619061) | 0.6696 | 0.503 | 2 |
Mn5O8 (mp-18922) | 0.6664 | 0.009 | 2 |
Li4FeBi(TeO6)2 (mp-776005) | 0.6562 | 0.036 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.6505 | 0.076 | 5 |
NaLiV(OF)2 (mp-764851) | 0.6961 | 0.078 | 5 |
Li4CrFe(WO6)2 (mp-770069) | 0.6797 | 0.174 | 5 |
Li4VFe(TeO6)2 (mp-761819) | 0.6887 | 0.060 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ba_sv Cr_pv O |
Final Energy/Atom-7.4989 eV |
Corrected Energy-236.9527 eV
Uncorrected energy = -209.9687 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.999 eV/atom x 8.0 atoms) = -15.9920 eV
Corrected energy = -236.9527 eV
|