material

CsSnI3

ID:

mp-616378

DOI:

10.17188/1277852


Tags: Cesium tin triiodide Cesium tin iodide - beta, HT

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.948 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.009 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.28 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CsSnI3
Band Gap
0.544 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mbm [127]
Hall
-P 4 2ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 69995 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <0 0 1> 0.001 155.5
PbSe (mp-2201) <1 0 0> <0 0 1> 0.002 77.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.003 311.0
BN (mp-984) <0 0 1> <1 0 1> 0.003 191.2
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.003 155.5
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.006 286.8
Au (mp-81) <1 1 0> <1 1 1> 0.006 221.2
CdS (mp-672) <1 0 0> <1 0 1> 0.006 286.8
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.007 233.3
GaSb (mp-1156) <1 0 0> <0 0 1> 0.008 77.8
Ag (mp-124) <1 1 0> <1 1 1> 0.009 221.2
ZnO (mp-2133) <1 1 0> <1 0 0> 0.014 333.7
CsI (mp-614603) <1 0 0> <0 0 1> 0.014 311.0
Au (mp-81) <1 0 0> <0 0 1> 0.014 155.5
CdSe (mp-2691) <1 0 0> <0 0 1> 0.015 77.8
SiC (mp-7631) <1 0 1> <1 0 0> 0.017 333.7
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.023 55.6
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.026 233.3
Cu (mp-30) <1 1 0> <1 0 0> 0.027 55.6
MgO (mp-1265) <1 0 0> <0 0 1> 0.027 311.0
Te2W (mp-22693) <0 0 1> <1 0 0> 0.027 111.2
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.042 166.9
C (mp-66) <1 0 0> <1 0 1> 0.048 191.2
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.048 236.0
Mg (mp-153) <0 0 1> <1 0 0> 0.050 278.1
SiC (mp-8062) <1 0 0> <0 0 1> 0.051 77.8
Mg (mp-153) <1 0 0> <1 0 0> 0.053 166.9
ZrO2 (mp-2858) <0 1 0> <1 1 1> 0.054 110.6
Ni (mp-23) <1 1 0> <1 0 0> 0.055 333.7
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.058 236.0
Ga2O3 (mp-886) <1 1 0> <1 0 0> 0.058 222.5
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.058 166.9
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.060 278.1
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.060 155.5
Si (mp-149) <1 1 0> <1 0 0> 0.061 166.9
ZnO (mp-2133) <1 0 1> <1 0 0> 0.064 278.1
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.069 77.8
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.071 95.6
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.071 314.6
Mg (mp-153) <1 1 0> <1 0 1> 0.071 286.8
ZnO (mp-2133) <1 1 1> <1 0 0> 0.073 222.5
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.074 77.8
TiO2 (mp-390) <0 0 1> <1 0 1> 0.078 286.8
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.083 311.0
C (mp-48) <1 0 1> <1 0 0> 0.084 333.7
InAs (mp-20305) <1 0 0> <0 0 1> 0.084 77.8
YAlO3 (mp-3792) <0 0 1> <1 0 1> 0.091 286.8
PbSe (mp-2201) <1 1 0> <1 0 0> 0.093 55.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.099 311.0
AlN (mp-661) <0 0 1> <1 1 0> 0.102 236.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
36 8 8 0 0 0
8 23 15 0 0 0
8 15 23 0 0 0
0 0 0 12 0 0
0 0 0 0 5 0
0 0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
30.8 -6.2 -6.2 0 0 0
-6.2 77.4 -48.3 0 0 0
-6.2 -48.3 77.4 0 0 0
0 0 0 85.6 0 0
0 0 0 0 200.5 0
0 0 0 0 0 200.5
Shear Modulus GV
8 GPa
Bulk Modulus KV
16 GPa
Shear Modulus GR
6 GPa
Bulk Modulus KR
16 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
16 GPa
Elastic Anisotropy
1.31
Poisson's Ratio
0.31

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
7.81 0.00 0.00
0.00 8.16 0.00
0.00 0.00 8.16
Dielectric Tensor εij (total)
7.99 0.00 0.00
0.00 8.16 0.00
0.00 0.00 8.16
Polycrystalline dielectric constant εpoly
(electronic contribution)
8.04
Polycrystalline dielectric constant εpoly
(total)
8.10
Refractive Index n
2.84
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeAlO3 (mp-4096) 0.1687 0.032 3
KMnF3 (mp-555359) 0.2021 0.000 3
NaTaO3 (mp-4675) 0.1853 0.005 3
EuTiO3 (mp-1079111) 0.1901 0.000 3
KMnF3 (mp-611990) 0.2007 0.000 3
SrTaNO2 (mp-552454) 0.2236 0.046 4
Sr2FeReO6 (mp-554620) 0.2180 0.000 4
Sr2NiMoO6 (mp-18940) 0.2254 0.000 4
Sr2GaSbO6 (mp-6304) 0.1623 0.026 4
Sr2FeMoO6 (mp-18857) 0.1832 0.183 4
Sr8Mg3Fe(MoO6)4 (mp-744025) 0.3169 0.054 5
Sr10Fe4Co(MoO6)5 (mp-745112) 0.2940 0.016 5
Sr20FeCo9(MoO6)10 (mp-706242) 0.2815 0.000 5
Na3SrTiNb3O12 (mp-695396) 0.3222 0.033 5
Sr20Fe9Co(MoO6)10 (mp-745210) 0.3322 0.000 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7383 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv Sn_d I
Final Energy/Atom
-2.8402 eV
Corrected Energy
-30.6761 eV
Uncorrected energy = -28.4021 eV Composition-based energy adjustment (-0.379 eV/atom x 6.0 atoms) = -2.2740 eV Corrected energy = -30.6761 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 262925
  • 69995
Submitted by
User remarks:
  • Cesium tin triiodide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)