Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.164 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPd7Se4 + Pd4Se |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 52.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 214.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 153.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 260.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 153.1 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 176.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 91.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 244.9 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 58.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 336.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 275.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 52.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 91.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 247.5 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 248.5 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 161.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 260.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 244.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 275.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 104.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 275.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 306.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 52.1 |
MoS2 (mp-1434) | <1 1 0> | <1 0 -1> | 117.5 |
Al (mp-134) | <1 0 0> | <0 1 0> | 215.0 |
Al (mp-134) | <1 1 1> | <0 1 1> | 247.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 91.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 246.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 260.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 260.7 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 156.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 153.1 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 275.6 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 153.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 -1> | 293.8 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 235.1 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 186.4 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 58.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 124.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 224.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 91.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 215.0 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 58.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 186.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 186.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 176.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 91.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeCu4Sn (mp-640286) | 0.6356 | 0.181 | 3 |
Mg6ZrC (mp-1022489) | 0.5814 | 0.703 | 3 |
CeMg6C (mp-1021162) | 0.6028 | 0.477 | 3 |
LaMg6B (mp-1099318) | 0.6156 | 0.368 | 3 |
CeMg6B (mp-1098076) | 0.5681 | 0.379 | 3 |
MgSi (mp-1073822) | 0.5717 | 0.192 | 2 |
Mg4Si3 (mp-1074349) | 0.5403 | 0.204 | 2 |
Mg3Si4 (mp-1075273) | 0.6054 | 0.230 | 2 |
Mg3Si2 (mp-1075818) | 0.6032 | 0.156 | 2 |
H3W (mp-1078686) | 0.6120 | 0.149 | 2 |
Rb (mp-640416) | 0.7077 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pd Se |
Final Energy/Atom-4.9672 eV |
Corrected Energy-89.4096 eV
-89.4096 eV = -89.4096 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)