Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.839 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbSe2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 0.001 | 200.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 0.001 | 137.1 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 0.003 | 168.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 0.005 | 221.4 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 0.006 | 200.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 0.007 | 126.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 0.010 | 192.0 |
WSe2 (mp-1821) | <1 0 0> | <1 1 1> | 0.012 | 251.4 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 0.013 | 192.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 0.014 | 221.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 0.015 | 137.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 0.015 | 196.6 |
YAlO3 (mp-3792) | <1 1 1> | <1 1 0> | 0.017 | 249.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 0.020 | 200.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 0.020 | 200.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 0.022 | 200.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 0.024 | 137.1 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 0.027 | 240.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 0.031 | 144.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 1 0> | 0.031 | 249.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 0.031 | 200.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 0.032 | 249.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 0.040 | 144.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 0.040 | 249.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 0.040 | 337.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 0.041 | 200.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 0.042 | 31.6 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 0.043 | 144.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 0.046 | 210.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 0.047 | 240.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 0.052 | 200.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 0.053 | 200.3 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 0.058 | 249.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 0.066 | 192.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 0.068 | 348.0 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 0.070 | 263.6 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 0.082 | 249.4 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 0.085 | 158.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 0.086 | 326.9 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 0.089 | 348.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 0.089 | 73.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 0.091 | 326.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 0.106 | 200.3 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 0.107 | 192.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 0.114 | 295.3 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 0> | 0.119 | 240.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 0.121 | 245.7 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 0.122 | 221.4 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 0.139 | 221.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 0.148 | 126.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
128 | 44 | 1 | 0 | 0 | 0 |
44 | 128 | 1 | 0 | 0 | 0 |
1 | 1 | 6 | 0 | 0 | 0 |
0 | 0 | 0 | 2 | 0 | 0 |
0 | 0 | 0 | 0 | 2 | 0 |
0 | 0 | 0 | 0 | 0 | 42 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.9 | -3.1 | -0.7 | 0 | 0 | 0 |
-3.1 | 8.9 | -0.7 | 0 | 0 | 0 |
-0.7 | -0.7 | 157.2 | 0 | 0 | 0 |
0 | 0 | 0 | 432.8 | 0 | 0 |
0 | 0 | 0 | 0 | 432.8 | 0 |
0 | 0 | 0 | 0 | 0 | 23.8 |
Shear Modulus GV24 GPa |
Bulk Modulus KV39 GPa |
Shear Modulus GR4 GPa |
Bulk Modulus KR6 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH23 GPa |
Elastic Anisotropy27.36 |
Poisson's Ratio0.24 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te8Mo3W (mp-1030155) | 0.3805 | 0.006 | 3 |
MoWS4 (mp-1030119) | 0.3795 | 0.002 | 3 |
Te4MoW (mp-1030106) | 0.3795 | 0.013 | 3 |
Te4MoW (mp-1029256) | 0.3811 | 0.013 | 3 |
MoW3S8 (mp-1029246) | 0.3803 | 0.002 | 3 |
MoWSe3S (mp-1030535) | 0.3864 | 0.113 | 4 |
MoWSe3S (mp-1030513) | 0.3911 | 0.096 | 4 |
Mo3W(Se3S)2 (mp-1027729) | 0.3892 | 0.056 | 4 |
Mo3W(Se3S)2 (mp-1080150) | 0.3817 | 0.073 | 4 |
MoW(SeS)2 (mp-1080170) | 0.3841 | 0.060 | 4 |
TaSe2 (mp-1071314) | 0.0203 | 0.004 | 2 |
TaSe2 (mp-637232) | 0.0190 | 0.005 | 2 |
NbSe2 (mp-7597) | 0.0479 | 0.001 | 2 |
TaSe2 (mp-1001742) | 0.0309 | 0.000 | 2 |
NbSe2 (mp-1072113) | 0.0391 | 0.003 | 2 |
Te4Mo3W(SeS)2 (mp-1030450) | 0.4860 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030404) | 0.4931 | 0.116 | 5 |
Te4Mo3W(SeS)2 (mp-1030284) | 0.4877 | 0.098 | 5 |
Te2MoWSeS (mp-1029213) | 0.4876 | 0.083 | 5 |
Te4MoW3(SeS)2 (mp-1028626) | 0.4924 | 0.111 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Se |
Final Energy/Atom-6.5367 eV |
Corrected Energy-39.2204 eV
-39.2204 eV = -39.2204 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)