Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.502 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.128 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrMnO3 + GeO2 |
Band Gap1.929 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 222.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 -1> | 283.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 -1> | 304.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 165.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 196.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 -1> | 289.6 |
AlN (mp-661) | <0 0 1> | <1 -1 1> | 211.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 169.9 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 86.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 253.7 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 1> | 264.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 126.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 156.9 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 173.4 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 86.7 |
GaN (mp-804) | <1 1 1> | <1 -1 1> | 211.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 274.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 278.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 196.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 285.4 |
GaN (mp-804) | <0 0 1> | <1 -1 -1> | 170.2 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 216.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 159.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 165.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.7 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 331.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 222.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 196.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 317.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 165.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 196.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 289.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 199.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 117.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 235.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 253.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 117.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 199.1 |
CdS (mp-672) | <0 0 1> | <1 -1 -1> | 227.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 159.3 |
CdS (mp-672) | <1 1 1> | <0 1 -1> | 206.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 117.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 117.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 196.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 325.9 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 222.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 -1> | 206.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaMoN3 (mp-989631) | 0.4901 | 0.000 | 3 |
SrTcN3 (mp-989627) | 0.5392 | 0.000 | 3 |
LaTcN3 (mp-989619) | 0.5218 | 0.000 | 3 |
CaGe2O5 (mp-554678) | 0.5535 | 0.014 | 3 |
Na2V2O5 (mp-1076048) | 0.5496 | 0.071 | 3 |
CaFeAsO5 (mvc-5813) | 0.4311 | 0.249 | 4 |
CaNiAsO5 (mvc-5683) | 0.4324 | 0.051 | 4 |
CaMnAsO5 (mvc-5587) | 0.4350 | 0.205 | 4 |
Li2Ni(PO3)4 (mp-761553) | 0.3686 | 0.069 | 4 |
NaV(GeO3)2 (mp-565634) | 0.4573 | 0.000 | 4 |
Nd3Al3Si3(NO6)2 (mp-695170) | 0.5041 | 0.006 | 5 |
CaScAlSiO6 (mp-39167) | 0.4884 | 0.000 | 5 |
SrCaCr(PO4)2 (mvc-3018) | 0.5690 | 0.185 | 5 |
Ca2MgAl2(SiO4)3 (mp-677029) | 0.5043 | 0.019 | 5 |
Na9LiFe10(SiO3)20 (mp-775304) | 0.5696 | 0.003 | 5 |
Na2Ca6Mg7Fe(SiO3)16 (mp-745155) | 0.5576 | 0.031 | 6 |
NaCaScZn(SiO3)4 (mp-684991) | 0.5696 | 0.019 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.5672 | 0.025 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.5531 | 0.031 | 6 |
Na5CaAl5Fe(SiO3)12 (mp-744927) | 0.5700 | 0.034 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Pr_3 Mn_pv Ge_d O |
Final Energy/Atom-7.2651 eV |
Corrected Energy-126.6260 eV
-126.6260 eV = -116.2414 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)