Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.917 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbFeF4 |
Band Gap2.887 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21212 [18] |
HallP 2 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 306.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 306.5 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 236.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 198.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 70.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 346.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 61.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 297.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 306.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 306.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 198.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 280.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 247.6 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 186.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 148.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 346.7 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 93.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 347.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 279.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 279.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 198.1 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 280.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 297.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 183.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 61.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 198.1 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 280.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 306.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 347.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 183.9 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 140.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 306.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 99.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 306.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 346.7 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 236.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 198.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 99.0 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 99.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 140.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 198.1 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 99.0 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 279.4 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 236.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 247.6 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 279.4 |
BN (mp-984) | <0 0 1> | <0 1 0> | 297.8 |
BN (mp-984) | <1 0 0> | <1 0 1> | 78.8 |
BN (mp-984) | <1 1 0> | <1 0 1> | 236.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 245.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsMnF4 (mp-616604) | 0.3850 | 0.198 | 3 |
CsTiF4 (mp-504701) | 0.4700 | 0.000 | 3 |
CsMnF4 (mp-617871) | 0.5460 | 0.250 | 3 |
CsFeF4 (mp-554225) | 0.3950 | 0.000 | 3 |
CsFeF4 (mp-605026) | 0.4889 | 0.000 | 3 |
MgSb2H2F14 (mp-849311) | 0.7350 | 0.000 | 4 |
CuSb2(XeF8)2 (mp-606617) | 0.7421 | 0.000 | 4 |
KNiAs3F18 (mp-566733) | 0.7121 | 0.009 | 4 |
Ba2FeCoF9 (mp-620091) | 0.7466 | 0.000 | 4 |
BiF5 (mvc-15798) | 0.5517 | 0.010 | 2 |
TaF5 (mvc-15779) | 0.5651 | 0.078 | 2 |
SbF5 (mvc-14697) | 0.5605 | 0.004 | 2 |
MoF5 (mvc-14217) | 0.5650 | 0.051 | 2 |
WF5 (mvc-14167) | 0.5684 | 0.028 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Rb_sv Fe_pv F |
Final Energy/Atom-4.9840 eV |
Corrected Energy-136.0314 eV
Uncorrected energy = -119.6154 eV
Composition-based energy adjustment (-0.462 eV/atom x 16.0 atoms) = -7.3920 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -136.0314 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)