Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.886 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.312 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 136.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 136.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 210.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 245.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 245.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 122.8 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 -1> | 136.6 |
C (mp-48) | <0 0 1> | <1 0 -1> | 136.6 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 245.5 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 1> | 183.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 245.5 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 122.8 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 122.8 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 149.6 |
Cu (mp-30) | <1 1 1> | <1 0 -1> | 136.6 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 -1> | 136.6 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 122.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd3NbO7 (mp-686043) | 0.7251 | 0.115 | 3 |
Ho3TaO7 (mp-676804) | 0.7470 | 0.129 | 3 |
Sr5(AlSb3)2 (mp-28392) | 0.6952 | 0.000 | 3 |
La5V3S6O7 (mp-650816) | 0.7399 | 0.060 | 4 |
TbCu(WO4)2 (mp-505190) | 0.7306 | 0.042 | 4 |
K2Mn(PS3)2 (mp-542638) | 0.7492 | 0.000 | 4 |
K4Sn(TeSe)2 (mp-569427) | 0.7273 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Sr_sv Al P |
Final Energy/Atom-4.4096 eV |
Corrected Energy-123.4689 eV
-123.4689 eV = -123.4689 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)