Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.754 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 125.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.0 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 300.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 325.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 303.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 281.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.9 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 281.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 156.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 250.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 155.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 225.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 303.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 217.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 156.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 325.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 62.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 303.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 300.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 325.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 162.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 94.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 225.4 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 225.4 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 303.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 344.6 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 162.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 94.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 207.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 313.2 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 250.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 259.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.9 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 344.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 187.9 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 94.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 207.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 52.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 156.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 281.9 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 281.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 219.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 156.6 |
BN (mp-984) | <1 0 1> | <1 1 0> | 217.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 103.9 |
BN (mp-984) | <1 1 1> | <1 0 1> | 303.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 207.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 281.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ErInRh (mp-3141) | 0.0266 | 0.000 | 3 |
ErInAu (mp-30375) | 0.0310 | 0.000 | 3 |
DyInAu (mp-22177) | 0.0248 | 0.000 | 3 |
HoInRh (mp-11104) | 0.0421 | 0.000 | 3 |
ErSnIr (mp-1078876) | 0.0353 | 0.000 | 3 |
Mg3Al9FeSi5 (mp-7062) | 0.6781 | 0.006 | 4 |
Tm3Mn3Ga2Si (mp-570450) | 0.7240 | 0.090 | 4 |
Mg3Al8FeSi6 (mp-571315) | 0.6970 | 0.141 | 4 |
Dy3Mn3Ga2Si (mp-21038) | 0.7299 | 0.322 | 4 |
U3Al3NiRu2 (mp-1080528) | 0.6460 | 0.088 | 4 |
USe2 (mp-8591) | 0.0997 | 0.032 | 2 |
Ti2P (mp-30218) | 0.2052 | 0.000 | 2 |
Mn2P (mp-1849) | 0.2604 | 0.000 | 2 |
K2Re (mp-1080778) | 0.1916 | 1.993 | 2 |
K2Tc (mp-1084834) | 0.2447 | 1.575 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv In_d Au |
Final Energy/Atom-4.9183 eV |
Corrected Energy-44.2644 eV
-44.2644 eV = -44.2644 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)