Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.232 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.631 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 249.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 114.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 83.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 249.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 83.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 231.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 166.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 83.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 154.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 231.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 114.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 166.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 308.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 166.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 231.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 231.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 249.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 166.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 166.2 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 231.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 231.2 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 114.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 83.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 249.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 229.8 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 249.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 249.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 83.1 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 83.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 308.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 231.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 77.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 166.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 154.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 308.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 166.2 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 114.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 154.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 229.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 1> | 229.8 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 166.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 83.1 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 154.2 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 83.1 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 166.2 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 249.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 154.2 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 83.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaYF5 (mp-777978) | 0.5361 | 0.097 | 3 |
BaYCl5 (mp-768965) | 0.5588 | 0.059 | 3 |
BaYI5 (mp-772077) | 0.5959 | 0.068 | 3 |
Ba2W2F11 (mvc-10059) | 0.6631 | 0.051 | 3 |
RhPb2F7 (mp-14276) | 0.6435 | 0.000 | 3 |
BaCaGaF7 (mp-8416) | 0.6226 | 0.000 | 4 |
Ba2CaCr2F14 (mvc-14958) | 0.4399 | 0.127 | 4 |
BaMnGaF7 (mp-622203) | 0.3995 | 0.005 | 4 |
BaCaCrF7 (mvc-16551) | 0.6208 | 0.067 | 4 |
Ba2ZnCu3F14 (mvc-1700) | 0.6108 | 0.000 | 4 |
Ba2CaMgAl2F14 (mp-540862) | 0.4743 | 0.000 | 5 |
Ba2CaCo2CuF14 (mvc-2242) | 0.6459 | 0.020 | 5 |
Ba2Mn2ZnCuF14 (mvc-2272) | 0.6228 | 0.133 | 5 |
Ba2CaTi2CuF14 (mvc-3436) | 0.5685 | 0.121 | 5 |
Ba2CaCuSn2F14 (mvc-2039) | 0.6078 | 0.133 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Cd Ga_d F |
Final Energy/Atom-4.8138 eV |
Corrected Energy-192.5534 eV
-192.5534 eV = -192.5534 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)