Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.275 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.090 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 1 0> | 251.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 251.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 194.0 |
BN (mp-984) | <0 0 1> | <1 1 1> | 197.0 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 194.0 |
C (mp-48) | <1 0 0> | <0 1 0> | 251.1 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 197.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 251.1 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 174.6 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 1> | 197.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 200.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te10Mo3I10 (mp-505260) | 0.5552 | 0.000 | 3 |
K3Mo3Se14 (mp-651347) | 0.6879 | 0.026 | 3 |
Re(TeBr2)2 (mp-662556) | 0.6659 | 0.000 | 3 |
Nb(Te2I3)2 (mp-570873) | 0.5547 | 0.000 | 3 |
Ag5CF4 (mp-29536) | 0.6362 | 0.248 | 3 |
TlRe6Se8Cl3 (mp-23635) | 0.6469 | 0.000 | 4 |
TlRe3(S2Cl)2 (mp-560005) | 0.7060 | 0.000 | 4 |
Gd3NbS3O4 (mp-510057) | 0.7170 | 0.020 | 4 |
NbTe2(SeI3)2 (mp-653891) | 0.5977 | 0.000 | 4 |
TlRe3(Se2Cl)2 (mp-23144) | 0.7127 | 0.001 | 4 |
Y8Co5 (mp-573425) | 0.7217 | 0.001 | 2 |
Mg3Si4 (mp-1075157) | 0.7007 | 0.187 | 2 |
Mg3Si4 (mp-1075482) | 0.7158 | 0.252 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv Br |
Final Energy/Atom-3.7362 eV |
Corrected Energy-149.4498 eV
-149.4498 eV = -149.4498 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)