@article{Yoshiasa1992, author = "Yoshiasa, A. and Takeno, S. and Iishi, K.", title = "Ba4In6O13: a compound with distorted square pyramidal InO5 coordination polyhedra", journal = "Mineralogical Journal (Japan)", year = "1992", volume = "16", pages = "40-48", ASTM_id = "MJTOAS" }