Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.369 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPr5Ga3 + Pr9Ga4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 253.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 345.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 230.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 253.9 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 85.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 230.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 203.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 203.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 253.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 172.7 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 307.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 245.6 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 307.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 256.1 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 256.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 230.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 245.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 253.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 274.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 137.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 274.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 241.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 172.7 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 245.6 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 203.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 172.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 103.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 68.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 203.1 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 230.4 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 153.6 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 230.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 253.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 307.0 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 184.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 274.4 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 203.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 230.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 205.8 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 245.6 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 203.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 152.3 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 307.0 |
BN (mp-984) | <0 0 1> | <1 0 1> | 76.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 241.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 241.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 256.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiSn5Rh3 (mp-638141) | 0.5655 | 0.000 | 3 |
Ni(TePd)2 (mp-12463) | 0.6155 | 0.000 | 3 |
Co(PdSe)2 (mp-12464) | 0.6531 | 0.000 | 3 |
Co(TePd)2 (mp-12465) | 0.6307 | 0.000 | 3 |
Fe(PdSe)2 (mp-12466) | 0.6161 | 0.008 | 3 |
Co2Si (mp-628766) | 0.5558 | 0.000 | 2 |
SnRh2 (mp-636334) | 0.5562 | 0.000 | 2 |
Mg2Hg (mp-30719) | 0.3808 | 0.003 | 2 |
Co2Si (mp-19905) | 0.5421 | 0.000 | 2 |
Ni2Ge (mp-17383) | 0.5453 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Ga_d |
Final Energy/Atom-4.5653 eV |
Corrected Energy-54.7832 eV
Uncorrected energy = -54.7832 eV
Corrected energy = -54.7832 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)