Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.440 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density17.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGaPt3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 139.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 215.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 153.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 132.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 187.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 161.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 53.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 107.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 307.9 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 250.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 153.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 215.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 153.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 246.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 215.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 176.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 277.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 278.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 153.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 309.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 220.9 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 139.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 153.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 153.9 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 277.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 44.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 153.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 132.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 187.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 220.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 153.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 215.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 246.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 176.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 107.7 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 53.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 246.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 338.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 88.4 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 215.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 44.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 215.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 338.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 107.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 92.4 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 269.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 220.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 246.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Zr (mp-1022517) | 0.3814 | 0.271 | 3 |
SrMg6W (mp-1016330) | 0.3889 | 0.348 | 3 |
KMg6W (mp-1099312) | 0.3754 | 0.427 | 3 |
KMg6W (mp-1098134) | 0.3855 | 0.428 | 3 |
Ce2Sn5 (mp-541131) | 0.4413 | 0.019 | 2 |
GaPt3 (mp-862621) | 0.3524 | 0.000 | 2 |
Ce3Sn7 (mp-28416) | 0.4408 | 0.000 | 2 |
La3Sn7 (mp-1079273) | 0.4508 | 0.000 | 2 |
AlPt3 (mp-1080448) | 0.3601 | 0.002 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d Pt |
Final Energy/Atom-5.7498 eV |
Corrected Energy-91.9961 eV
-91.9961 eV = -91.9961 eV (uncorrected energy)
|